Full text
PROJECTE O TESINA D’ESPECIALITAT Títol NUMERICAL ANALYSIS OF THE OUT-OF-PLANE BEHAVIOR OF UNREINFORCED MASONRY WALLS Autor/a LAURA SENDRA GONZÁLEZ Tutor/a ANTONIO RODRÍGUEZ FERRAN, LUKAS REINDL Departament MATEMÀTICA APLICADA III Intensificació ENGINYERIA COMPUTACIONAL Data 01/07/2010
Títol NUMERICAL ANALYSIS OF THE OUT-OF-PLANE BEHAVIOR OF UNREINFORCED MASONRY WALLS Autor/a LAURA SENDRA GONZÁLEZ Tutor/a ANTONIO RODRÍGUEZ FERRAN, LUKAS REINDL Especialitat ENGINYERIA COMPUTACIONAL Data 01/07/2010 Resum Out-of-plane stability of unreinforced masonry walls is an important aspect to be taken into account in edification. This construction technique is widely used and it is one of the most vulnerable to seismic loading. It has been observed that damage produced by out-of-plane loadings is one of the most commonly produced failure mechanisms in seismic hazards. Despite of that, research into the out-of-plane stability of masonry walls is not yet enough developed. The aim of this research is to create a three-dimensional finite element model in order to study the latter problem. A parametrical study is performed on two numerical models under monotonic and cyclic out-of-plane loads. The influence of various geometrical and boundary
conditions are studied in two different models of a single wall: a homogenized and a distinct model. A damage plasticity formulation, appropriate for brittle materials, is implemented for modeling the behavior of the wall. In the distinct model, frictional and cohesive interaction models are used for modeling the joints, which are constituted by mortar. Firstly a monotonic homogeneous distributed out-of-plane pressure is applied, in order to determine both, the resistance of the wall in terms of its force-displacement curve, and the failure mechanism. Next, the same model is submitted to cyclic out-of-plane uniform pressure and energy dissipation, as well as stiffness degradation is analyzed. Finally, some qualitative recommendations for the unreinforced masonry walls are derived from the results, with the purpose of maximizing the resistance in front of out-of-plane loading.
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls Contents List of figures ............................................................................................................................ 3 List of tables ............................................................................................................................. 6 Nomenclature .......................................................................................................................... 7 Abstract .................................................................................................................................... 9 Resumen................................................................................................................................. 11 1. Introduction ................................................................................................................ 13 1.1. State-of-the-Art .............................................................................................................. 13 1.2. Aim and work configuration ........................................................................................... 14 2. Non-linear model “Concrete Damage Plasticity” for masonry ................................... 15 2.1. Concrete damaged plasticity formulation ...................................................................... 15 2.2. Material model calibration and analysis ........................................................................ 20 3. Process for the non-linear analysis of URMW ............................................................ 29 3.1. Solution technique ......................................................................................................... 29 3.1.1. Finite element formulation ....................................................................................... 29 3.1.2. Method of modeling ................................................................................................. 30 3.2. Analysis process.............................................................................................................. 31 3.2.1. Pre-processing – Abaqus/CAE ................................................................................... 31 3.2.2. Processing ................................................................................................................. 32 3.2.3. Post-processing ......................................................................................................... 32 4. Homogeneous Unreinforced Masonry Wall Study ..................................................... 33 4.1. Description of the model ................................................................................................ 34 4.1.1. Geometry .................................................................................................................. 34 4.1.2. Contact Modeling ...................................................................................................... 35 4.1.4. Out-of-plane load ...................................................................................................... 37 4.2. Wall A ............................................................................................................................. 37 4.2.1. Results and discussion ............................................................................................... 37 4.3. Walls E and I ................................................................................................................... 42 4.3.1. Confinement of the wall ............................................................................................ 43 4.3.2. Wall E ......................................................................................................................... 44
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 2 4.3.3. Wall I.......................................................................................................................... 48 4.3.4. Overall comparison: influence of the boundary conditions ..................................... 52 4.4. Conclusions ..................................................................................................................... 53 4.5. Different meshing schemes ............................................................................................ 54 5. Detailed Unreinforced Masonry Wall ......................................................................... 57 5.1. Preliminary study of contact between bricks ................................................................. 57 5.1.1.1. Tangential contact behavior: friction model ............................................................. 57 5.1.1.2. Normal contact behavior .......................................................................................... 60 5.1.2. Numerical simulations ............................................................................................... 62 5.2. Numerical model of a detailed UMW under monotonic out-of-plane loading ............. 66 5.2.1. Numerical results and discussion .............................................................................. 66 5.3. Comparison between the Homogenized and Detailed walls ......................................... 74 5.4. Validation of the model .................................................................................................. 75 5.5. Unreinforced Masonry Wall under quasi-static cyclic out-of-plane loading ................. 78 6. Conclusions ................................................................................................................. 87 7. References ................................................................................................................... 89
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 3 List of figures Figure 1 Tensile and compressive postfailure behavior ............................................................. 16 Figure 2 Uniaxial load cycle tension-compression-tension ........................................................ 17 Figure 3 Yield surface in plane stress .......................................................................................... 20 Figure 5 Numerical result of the simple tensile test ................................................................... 22 Figure 4 Cylindrical sample. ........................................................................................................ 22 Figure 6 Numerical results of the simple compressive test ........................................................ 23 Figure 7 Numerical results of the cyclic test ............................................................................... 24 Figure 9 Comparison between experimental data and numerical results of TPB Test ............... 25 Figure 8 Prismatic sample. . ........................................................................................................ 25 Figure 10 Crack propagation in the three point bending test ..................................................... 26 Figure 12 Stress - cracking displacement descriptions used in the curve-fitting procedure ...... 27 Figure 11 Cracking propagation direction in the three point bending test ................................ 27 Figure 13 Three point bending test results in the curve-fitting procedure ................................ 28 Figure 14 Analysis steps .............................................................................................................. 31 Figure 15 Homogenization technique [19].................................................................................. 33 Figure 16 Geometry of walls A, E and I. Wall A has three fixed edges and the top free edge ... 34 Figure 17 Plastic strain distribution in absence of concrete frame ............................................ 35 Figure 18 Comparison of the deformed shape depending on the contact formulation used .... 36 Figure 19 Influence of the aspect ratio ....................................................................................... 38 Figure 20 Influence of thickness .................................................................................................. 38 Figure 21 Influence of vertical load level .................................................................................... 39 Figure 22 Failure pattern for yield-line, fracture-line and failure-line theories [20] .................. 40 Figure 23 Plastic strains at ultimate state for wall A ................................................................... 41 Figure 24 Two-way bending cracking pattern [4] ....................................................................... 41 Figure 25 Stress distribution at steps 1 (a) and 4 (b) .................................................................. 42 Figure 26 Stress distribution at steps 6 (a) and 12 (b) ................................................................ 42 Figure 27 Stress distribution at steps 13 (a) and 14 (b) .............................................................. 42 Figure 28 Comparison between stresses due to displacement and increment of temperature 43 Figure 29 Influence of the aspect ratio in wall E ......................................................................... 44 Figure 30 Influence of thickness in wall E ................................................................................... 45 Figure 31 Plastic strains at ultimate state in wall E at steps 7 and 14 ........................................ 46 Figure 32 Two-way bending cracking pattern [6] ....................................................................... 46 Figure 33 Stress state at steps 5 (a) and 8 (b) ............................................................................. 47 Figure 34 Stress state at steps 11 (a) and 14 (b) ......................................................................... 47 Figure 35 Stress-plastic strain in the most tensed point ............................................................. 47 Figure 36 Influence of the aspect ratio in wall I .......................................................................... 48 Figure 37 Influence of thickness in wall I .................................................................................... 49 Figure 38 Plastic strains at initial state (a) and ultimate state (b) on wall I ................................ 50 Figure 39 Stress states at steps 1 (a) and 8 (b) ........................................................................... 50 Figure 40 Stress state at steps 15 (a) and 20 (b) ......................................................................... 50 Figure 41 Stress state at steps 25 (a) and 34 (b) ......................................................................... 51
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 4 Figure 42 Stress-plastic strain curve in the most compressed point of wall............................... 51 Figure 43 Stress - Plastic strain curve in the most tensed point ................................................. 52 Figure 44 Influence of the boundary conditions ......................................................................... 52 Figure 45 Coarse, medium and fine meshes used in the convergence test ............................... 54 Figure 46 Comparison of the results for meshes ........................................................................ 54 Figure 47 Relative error committed with coarse and medium meshes analyses ....................... 55 Figure 48 Load and unload shear tests versus horizontal shear displacement .......................... 59 Figure 49 Expected tangential behavior ..................................................................................... 59 Figure 50 Typical traction-separation response in the cohesive model ..................................... 61 Figure 51 Influence of the contact formulation in the simple shear test ................................... 62 Figure 52 Shear-relative displacement and traction-separation displacement .......................... 63 Figure 53 Influence of cohesion between bricks on the wall sample ......................................... 64 Figure 54 Stress states and plastic strains in the wall sample without cohesion ....................... 65 Figure 55 Stress states and plastic strains in the wall sample with cohesion ............................. 65 Figure 56 Numerical model of the detailed masonry wall .......................................................... 66 Figure 57 Influence of the aspect ratio in the detailed model .................................................... 67 Figure 58 Influence of the thickness of the wall in the detailed model ...................................... 67 Figure 59 Influence of the vertical load level in the detailed model .......................................... 68 Figure 60 Influence of the boundary conditions of the detailed wall ......................................... 69 Figure 61 Stress states of the detailed model A at steps 7 and 9 ............................................... 69 Figure 62 Stress- Plastic strain in the most compressed point ................................................... 70 Figure 63 Plastic strains of wall A at different steps: when they appear, ................................... 70 Figure 64 Stress Plastic strain in the most compressed point (a) and ........................................ 71 Figure 65 Plastic strains of detailed wall I at different steps ...................................................... 71 Figure 66 Stress- Plastic strain in the most compressed point ................................................... 72 Figure 67 Stress states of detailed wall I at different steps ........................................................ 72 Figure 68 Comparison between homogenized and detailed models ......................................... 74 Figure 69 Comparison between the homogenized and the detailed model .............................. 74 Figure 70 Failure mechanism in the experimental test .............................................................. 76 Figure 71 Geometry and mesh of the model used for verification ............................................. 76 Figure 72 Comparison between experimental and numerical results ........................................ 77 Figure 73 Deformation in the out-of plane direction (a) and plastic strains (b) ......................... 78 Figure 74 Calculation of the equivalent viscous damping........................................................... 79 Figure 75 Out-of-plane loading history in the cyclic test for wall A ............................................ 80 Figure 76 Hysteretic response of wall A under cyclic test .......................................................... 81 Figure 77 Stress - Plastic strain developed in the most solicited point of wall A ........................ 81 Figure 78 Force-displacement response of the wall under out-of-plane cyclic load .................. 82 Figure 79 Stress - Plastic strain of most solicited point of wall I subjected to cyclic loading ..... 83 Figure 80 Hysteretic response of wall Aa under cyclic test......................................................... 83 Figure 81 Stress - Plastic strain in the most solicited point of wall Aa under cyclic test ............ 84 Figure 82 Hysteretic response of wall Ab under cyclic test ........................................................ 84 Figure 83 Stress evolution developed in the most solicited point of wall Ab ............................. 85
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 5
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 6 List of tables Table 1 Compressive crushing behavior...................................................................................... 21 Tabla 2 Tensile cracking behavior ............................................................................................... 21 Table 3 Compressive damaged behavior .................................................................................... 23 Table 4 Tensile damaged behavior.............................................................................................. 23 Table 5 Stress-cracking strain description ................................................................................... 25 Table 6 Tensile cracking behavior ............................................................................................... 28 Table 7 General analysis options ................................................................................................. 31 Table 8 Material properties used in the wall models ................................................................. 34 Table 9 Combination for the wall with top free edge ................................................................. 37 Table 10 Totally hinged wall combinations ................................................................................. 44 Table 11 Combination of walls for BC I ....................................................................................... 48 Table 12 Wall properties for the influence of boundary conditions ........................................... 52 Table 13 Characteristics of the mesh used in the study of convergence.................................... 54 Table 14 Sliprate dependent data for the friction coefficient .................................................. 59 Table 15 Stiffness coefficients ..................................................................................................... 61 Table 16 Combinations of the detailed model ............................................................................ 66 Table 17 Material properties of brick and bond in the experimental tests ................................ 75
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 13 1. Introduction 1.1. State-of-the-Art Unreinforced masonry is a construction technique widely used in edification constructions and one of the most vulnerable to seismic loading. It has been observed that damage produced by out-of-plane loadings is one of the most commonly observed failure mechanisms in seismic hazards. Despite of that, research into the out-of-plane stability of masonry walls is not yet enough developed and very simplified construction rules based on slenderness criteria and geometric properties are used as design criteria. Moreover, whilst a considerable amount of effort has been conducted on one-way vertically spanning walls [1], current understanding of the seismic response of two-way walls is still limited. One of the main future goals of the research into masonry is a more accurate approach for the out-of-plane design of masonry walls. Research on the latter problem is performed by means of experimental and analytical investigations, which can be carried out from different points of view. In order to create proper design methodologies as well as to enhance the theoretical knowledge about the matter, static, quasi-static and dynamic analyses have been performed in the past years. Models have been built with different geometrical and structural characteristics to study the corresponding parametrical influence [2], as well as comparisons to analytical predictions of simplified models based on limit state analysis for materials such masonry [2]. Laboratory tests conducted on walls subjected to monotonic loading show how failure takes place along regular pattern of lines whose arrangement depends on boundary conditions and aspect ratio [3]. That has inspired approximation methods based on fracture line theory [4]. Stress state and stiffness degradation of masonry walls during the process of damage vary with material layout, so that is difficult to obtain reliable mathematical models [5]. Displacement-based design has become popular in the recent years for ductile structural systems assessment, such as multi-storey buildings [6], but its level of development is not as high as in the in-plane stability problem. It has been observed that the displacement-based method gives significantly better predictions than the force-based method, which moreover, cannot be used in some cases. Recently, a simplified displacement-based design procedure for vertically spanning walls has been developed [7], by using a trilinear relationship to approximate the nonlinear loaddisplacement behavior. The investigation uses a single degree of freedom analytical model to extend the analytical database on dynamic URMW behavior. Experimental tests have been carried out for a wide range of wall geometries, boundary conditions, gravity loading and ground motion characteristics, in order to verify the method’s accuracy by quasi-static cyclic tests [8] on full-scale specimens and by dynamic tests on half
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 14 scale specimens subjected to harmonic sinusoidal acceleration at resonance frequency and to realistic seismic input [9]. Computer simulations have been used as a tool to reduce the research economic cost. By this tool, investigations on the sensitivity of the peak dynamic displacement response to hysteresis modeling parameters [9] and system properties have been carried out [10]. Finite element studies of an URMW panel based on a discrete cracking model, using elastic volume elements to model masonry material, and surface contact elements to model mortar joints [11]. While two way bending analysis are limited [3] experimental and analytic studies in one way span conditions are abundant [12]. 1.2. Aim and work configuration In order to study the concerning problem of this thesis a finite element model of a masonry wall will be developed as three-dimensional solid. The finite element analysis of this thesis is performed by using Abaqus/Standard program. Abaqus/Standard is a finite element program with a wide range of material models, in particular for brittle materials, such as concrete and masonry, as well as contact formulations, which, in a detailed model of a masonry wall, can be implemented to define the interaction between bricks. For this reason, Abaqus is preferred to Ansys, which does not provide as many material options, and which is usually used in the Department of Statics and Dynamics of the RWTH-Aachen University. In this thesis, a calibration of the material is performed by the adjustment of the behavior of modeled samples of calcium silicate to experimental data. In a second stage, a homogeneous unreinforced wall is modeled and its behavior under monotonic out-of-plane loading is studied. The influence of different boundary conditions, vertical load levels and brick and wall geometries is analyzed. In a further stage a detailed unreinforced model is developed and, by a similar procedure, a parametrical study is performed, as well as a study on the influence of different bond designs. Finally, a quasi-static cyclic analysis is performed on the detailed model.
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 2. Non-linear model “Concrete Damage Plasticity” for masonry Abaqus/Standard provides two models for non-linear brittle materials behavior, smeared cracking and concrete damaged plasticity. The material model concrete damaged plasticity in Abaqus/Standard is based on isotropic damaged elasticity in combination with isotropic tensile and compressive plasticity to represent inelastic behavior of concrete. This material model is designed for elements subjected to arbitrary loadings, such as cyclic loadings. For this reason, this material model is preferred for seismic analyses of masonry structures. 2.1. Concrete damaged plasticity formulation Concrete damaged plasticity model assumes that the brittle material, unreinforced masonry in this case, fails due to two main failure mechanisms: tensile cracking and compressive crushing. The evolution of the yield surface (or failure) is determined by two hardening variables, tensile equivalent plastic strain ( pl t ε ~ ) and equivalent compressive plastic strain ( pl c ε ~ ), linked to the tension and compression failures respectively. This model assumes that failure of masonry can be effectively modeled using its response to uniaxial tension, uniaxial compression and by the plasticity characteristics. Under uniaxial tension, the stress-strain response follows a linear elastic relationship until the yield stress value. When the failure stress is reached, micro cracking formation in masonry is assumed to begin. Beyond the failure stress, the formation of micro-cracks is represented macroscopically with a softening stress-strain response, which induces strain localization in the structure. Under uniaxial compression, the response remains linear until the initial value of yield stress is reached. In the plastic regime, the response is typically characterized by stress hardening followed by strain softening. In addition to the compressive and tensile stress-strain data, this material model requires five parameters to define Drucker-Prager plastic flow function and yield function proposed by Lubliner [13]. These parameters are the dilation angle, flow potential eccentricity, ratio of initial equi-biaxial compressive yield stress to initial uniaxial compressive yield stress (σ bo /σ co ) and the ratio of the second stress invariant on the tensile meridian to that on the compressive meridian. The value of dilation angle for calcium silicate is set equal to 36° and due to the lack of experimental data, the default values for the other parameters are adopted: 0.1, 1.16 and 0.67 respectively. Tensile postfailure behavior of masonry is modeled with tension stiffening, in terms of the strain-softening behavior. Tension stiffening can be described by means of a postfailure stressstrain relationship or by applying a fracture energy cracking criterion. Both descriptions are
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 16 studied. Postfailure stress is given as a function of cracking strain, defined as the total strain minus elastic strain: el t t ck t 0 εεε −= , where 0 / 0 E t el t σε = (1 ) If unloading data are available, they can be introduced in the model in terms of tensile damage curves, ck tt d ε − , so that the cracking strain values are converted to plastic strain values by: ( ) 0 1 ~Et t d t d ck t pl t σ εε − −= (2) In a similar way as in the tensile postfailure behavior, compressive stress data are provided as a tabular function of inelastic (or crushing) strain. The stress-strain curve is defined beyond the yield stress, into the softening range. Hardening data are given in terms of an inelastic strain, defined as the total strain minus the elastic strain corresponding to the undamaged material: el c c in c 0 εεε −= , where 0 0Ec el c σ ε = (3) If unloading data are available, they can be introduced in the model in terms of tensile damage curves, in c c d ε − , so that the cracking strain values are converted to plastic strain values by: ( ) 0 1 ~Ec c d c d in c pl c σ εε − −= (4) Figure 1 Tensile and compressive postfailure behavior [14] Under uniaxial cyclic loading conditions the degradation mechanisms are quite complex, involving the opening and closing of previously formed micro-cracks, as well as their interaction. Experimentally, it is observed that there is some recovery of the elastic stiffness as the load changes sign during a uniaxial cyclic test. The stiffness recovery effect, also known as the “unilateral effect,” is an important aspect of the concrete behavior under cyclic loading. The effect is usually more pronounced as the load changes from tension to compression, causing tensile cracks to close, which results in the recovery of the compressive stiffness.
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 17 The concrete damaged plasticity model assumes that the reduction of the elastic modulus is given in terms of a scalar degradation variable d as: ( ) o EdE −= 1 (5) where E 0 is the initial (undamaged) modulus of the material. This expression holds both in the tensile and the compressive sides of the cycle. The stiffness degradation variable, d, is a function of the stress state and the uniaxial damage variables. For the uniaxial cyclic conditions: ( ) ( ) ( ) t d c s c d t sd −−=− 111 (6) where s t and s c are functions of the stress state that are introduced to model stiffness recovery effects associated with stress reversals. ( ) ( )( ) 1 c w0 ; 11 *11 1 t w0 ; 11 *1 ≤≤−−= ≤≤−= σ σ r c w c s r t w t s (7) where ( ) ( ) < > == 0 11 if 0 0 11 if 1 1111 * σ σ σσ Hr (8) the weight factors w t and w c , which are assumed to be material properties, control the recovery of the tensile and compressive stiffness upon load reversal. The experimental observation in most quasi-brittle materials is that the compressive stiffness is recovered upon crack closure as the load changes from tension to compression. On the other hand, the tensile stiffness is not recovered as the load changes from compression to tension once crushing micro-cracks have developed. This behavior corresponds to w c =1 and w t =0, which are assumed in the calculations. Figure 2 Uniaxial load cycle tension-compression-tension [14]
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 18 Concrete plasticity is defined in Abaqus/Standard through the flow potential, yield surface and viscosity parameters. The stress-strain relations for the general three-dimensional multiaxial condition are given by the scalar damage elasticity equation: ( ) −−= pl el Dd εεσ : 0 1 (6) where D 0 el is the initial (undamaged) elasticity matrix and the scalar stiffness degradation variable, d, is generalized to the multiaxial stress case. The plastic flow potential function and the yield surface make use of two stress invariants of the effective stress tensor, namely the hydrostatic pressure stress, ( ) σ 3 1tracep −= (7) and the Mises equivalent effective stress, ( ) SSq : 2 3 = (8) where S is the effective stress deviator, defined as IpS += σ (9) The effective stress is defined as ( ) plel D εεσ −= : 0 (10) The model assumes nonassociated potential plastic flow. The flow potential G used for this model is the Drucker-Prager hyperbolic function: ( ) ψψξσ tantan 2 2 0 pqG t −+= (10) where ( ) i f, θ ψ (11) is the dilation angle measured in the p–q plane at high confining pressure. ( ) 0 ~ , = = pl t tito f ε σθσ (12) is the uniaxial tensile stress at failure, taken from the user-specified tension stiffening data and ( ) i f, θ ξ (13)
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 19 is a parameter, referred to as the eccentricity, that defines the rate at which the function approaches the asymptote (the flow potential tends to a straight line as the eccentricity tends to zero). This flow potential, which is continuous and smooth, ensures that the flow direction is always uniquely defined. The function approaches the linear Drucker-Prager flow potential asymptotically at high confining pressure stress and intersects the hydrostatic pressure axis at 90°. The default flow potential eccentricity is x=0, which implies that the material has almost the same dilation angle over a wide range of confining pressure stress values. Increasing the value of x provides more curvature to the flow potential, implying that the dilation angle increases more rapidly as the confining pressure decreases. The model makes use of the yield function of Lubliner [13], with the modifications proposed by Lee and Fenves [15] to account for different evolution of strength under tension and compression. The evolution of the yield surface is controlled by the hardening variables, pl t ε ~ and pl c ε ~ . In terms of effective stresses, the yield function takes the form: ( ) ( ) ( ) 0 ~ ˆˆ ~ 3 1 1 maxmax =−−−+− − = pl cc pl pqF εσσγσεβα α (14) with ( ) ( ) ( ) ( ) ( ) ( ) ( ) 12 13 11 ~ ~ 0.50 ; 1/2 1/ t c 00 00 − − = +−−= ≤≤ − − = c c pl t pl c cb cb K K γ αα εσ εσ β σ σσ σ σ α (15) (16) (17) where, max ˆ σ is the maximum principal effective stress; ( ) 00 / cb σσ is the ratio of initial equibiaxial compressive yield stress to initial uniaxial compressive yield stress (the default value is 1.16); K c is the ratio of the second stress invariant on the tensile meridian, 0 max < σ and it must satisfy the condition 0.5<K c <1.0 (the default value is 2/3). ( ) pl tt εσ ~ is the effective tensile cohesion stress; and ( ) pl cc εσ ~ is the effective compressive cohesion stress.
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 20 Figure 3 Yield surface in plane stress [14] Box 1 Summary of the Concrete Damage Plasticity material model 1. Constitutive equation: ( ) ( ) plel Dd εεσ −−= :1 0 2. Plastic flow: ( ) ψψξσ tantan 2 2 0 pqG t −+= 3. Yield function: ( ) ( ) ( ) 0 ~ ˆˆ ~ 3 1 1 maxmax =−−−+− − = pl cc pl pqF εσσγσεβα α Where the parameters , , , 0 dD plel ε pq t , , , , 0 ψ σ ξ pl c εγσβα ~ , , ˆ , , , max have been defined in the preceding equations. 2.2. Material model calibration and analysis The material model has to be tested and adjusted to the special requirements of masonry using experimental testing results. Masonry object of this study is made of calcium silicate bricks and mortar. The experimental data [16] provided by the Institute of experimental tests
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 21 for construction investigations of the RWTH-Aachen University contains information about the stress-strain curves of cylindrical calcium silicate samples under simple tension and simple compression experiments, as well as the force-displacement curve of a prismatic sample under bending, obtained in the three point bending test. These experimental tests are modeled numerically. 2.2.1. Material data A first approach is made in order to assess the behavior of the model depending on the inputted parameters. The material data used is a simplification of the experimental behavior of tested calcium silicate samples [16]. The elastic behavior is modeled as isotropic, with elastic modulus equal to 9 GPa and Poisson ratio equal to 0.12. The plastic behavior of the material is initially modeled by data of tables 1 and 2. Table 1 Compressive crushing behavior Compressive behavior Crushing stress (MPa) Plastic strain 10 0 15 0.0007 18 0.0017 20 0.0027 19 0.0037 16 0.0047 15 0.0049 Tabla 2 Tensile cracking behavior Tensile behavior Cracking stress (MPa) Plastic strain 2 0 1 . 3 0. 0001 0. 9 0. 0002 0. 6 0. 0003 0. 4 0. 0004 0. 26 0. 0005 0. 23 0. 0006 0. 21 0. 0007 0. 2 0. 0008 0. 25 0. 0085 0.0 2 0. 01
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 22 2.2.2. Cylindrical sample subjected to simple tension and compression 2.2.2.1 Simple Tensile Test A cylindrical sample with the same configuration as in the experimental test is subjected to incremental displacements on its upper face. A displacement based analysis is carried out in order to observe the entire behavior of the sample under tension. The cylinder is subjected on its entire lower face. As the subjection conditions in the experimental test might be slightly different, thus not perfect, some variations on the results are expected. The numerical results are shown in figure 5. Figure 5 Numerical result of the simple tensile test As expected, the material behaves elastically until the yield point, reached at 2 0 = t σ MPa. In the post peak behavior, the softening governs the behavior of the sample. The tensile behavior is described for a range of strain wide enough to allow the model to work, when tension and compression happen simultaneously, even if the tensed fibers have already overcome the yield point and softened. 0,00 0,50 1,00 1,50 2,00 2,50 0 0,0005 0,001 0,0015 0,002 0,0025 Stress (MPa) Strain Figure 4 Cylindrical sample. Diameter: 80 mm. Length: 160 mm. Fixed on its lower face and subjected to displacements on the upper face
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 29 3. Process for the non-linear analysis of URMW In this section, the procedure followed in all the numerical simulations done in this thesis is specified in a general way. 3.1. Solution technique In non-linear problems, the objective is to obtain a convergent solution at a minimum cost. For this purpose, the problem history is divided into steps, which correspond to any convenient phase of the experiment, for example, it is a change of the load or displacement’s magnitude. By using automatic control, the step, the tolerances and error measures can be defined by the user, but the increment size is chosen by the program depending on the response of the model in the step. This technique is known as adaptive load-stepping. 3.1.1. Finite element formulation The finite element models generated in the concerning study are nonlinear and involve a large amount of variables. In terms of these variables the equilibrium equations obtained by discretizing the virtual work equation can be written symbolically as: ( ) 0= MN uF (18) where F N is the force component conjugate to the N th variable in the problem and u M is the value of the M th variable. The basic problem is to solve equation 18 for the u M throughout the history of interest. Newton’s method is used as a numerical technique for solving the nonlinear equilibrium equations, due to its convergence rate compared to the convergence rates exhibited by alternate methods (such as modified Newton or quasi-Newton methods). Newton’s method can be formally described as follows. Assume that, after an iteration i, an approximation u i M , to the solution has been obtained. Let c i+1 M be the difference between this solution and the exact solution to the discrete equilibrium equation. This means that: ( ) 0 1 =+ +M i M i N cuF (19) expanding the left-hand side of this equation in Taylor series about the approximate solution u i M , ( ) ( ) ( ) 0... 11 2 1 =+++ +++ Q i P i M i QP N P i M i P N M i N ccu u u F cu u F uF δδ δ δ δ (20) If u i M is a close approximation to the solution, the magnitude of each c i+1 M will be small, and so all but the first two terms above can be neglected giving a linear system of equations: N i P i NP i FcK −= +1 (21)
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 30 where ( ) M i P N NP i u u F K δ δ = (22) is the Jacobian matrix and ( ) M i NN i uFF = (23) the next approximation to the solution is then M i M i M i cuu 11 ++ += (24) and the iteration continues. Convergence of Newton’s method is best measured by ensuring that all entries in F i N and all entries in c i+1 N are sufficiently small. Both these criteria are checked by default by the program in the solution. 3.1.2. Method of modeling Static general analysis procedure Static general analysis is used. In this non-linear analysis type inertia effects are neglected and time-dependent material effects are ignored. Automatic stabilization method (by default with dissipated energy fraction equal to 2.0E-4) is used, so that local instabilities are stabilized by applying damping throughout the model. Incrementation in the steps The time increments are chosen automatically by the program depending on the computational efficiency. The maximum number of increments is, in the majority of the steps, 100, so that the analysis stops if this maximum is exceeded before arriving to the complete solution for the step. The minimum increment is usually set to 1E-7, and if the program needs a smaller time increment, it terminates the analysis. Equation solver method A direct equation solver is implemented and the matrix storage of the solution scheme is unsymmetric, according to the requirements of the material properties of the model Concrete damaged plasticity. Element Type Three dimensional linear and hexahedral solid elements are used in the discretization of the model. The element type C3D8R (8 node linear brick with reduced integration and hourglass control) is used in all the models. The corresponding element controls are summarized in table 7.
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 31 Table 7 General analysis options Reduced integration No hybrid formulation, no incompatible modes Hourglass stiffness By default: an additional artificial stiffness is added to the element Viscosity By default, a small value for viscosity parameter is used to improve the rate of convergence of the model in the softening regime without compromising results. Kinematic split Average strain Second-order accuracy No Distortion control By default. It prevents the elements form exceeding the deformation ratio Element deletion and maximum degradation By default, the elements where the failure criterion is locally reached, are removed from the calculation 3.2. Analysis process The following flow diagram shows the steps undertaken during the analysis. Figure 14 Analysis steps 3.2.1. Pre-processing – Abaqus/CAE The steps followed to create the numerical models with Abaqus/CAE are listed below: 1. Create basic elements by describing their geometrical properties. a. Macro model: homogeneous masonry wall and concrete frame. b. Detailed model: bricks and concrete frame. 2. Create material properties for the bricks or homogeneous wall (Calcium silicate and concrete) 3. Create the assembly of the elements (relative position) and assign them their material properties. 4. In the models in which contact appears: Create contact properties and assign them to the different pairs of surfaces in contact. 5. Create the mesh and select the element type 6. Create the steps 7. Create the boundary conditions and loads 8. Create an output data request 9. Create a job Pre-processing Processing Postprocessing Results acceptable and solution stable Plot output results
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 32 3.2.2. Processing During the processing phase, the stress-strain states are checked along the analysis in order to identify possible problems of convergence during calculations. When they are not acceptable, the step size is changed, until the analysis can proceed until its end. 3.2.3. Post-processing The results are taken from the .odb file for each job: load-displacement response of the model along the history of the analysis, stress-strain state and maximum plastic strain directions at different time points of the analysis. The load is measured as the sum of the reaction forces at the nodes in which the boundary conditions are applied and the displacement is measured at the most deformed element in each case. The evolution of the stress-strain state gives information about the loading distribution along the analysis and the maximum plastic strain direction distribution shows the crack formation, thus, the failure mechanism mode.
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 33 4. Homogeneous Unreinforced Masonry Wall Study Masonry is an orthotropic composite structure constituted by bricks and mortar in which mortar joints can behave as planes of failure. The average material properties can be derived from experimental tests with a composite specimen or from a numerical reproduction of the masonry behavior [18, 19]. Nevertheless, masonry structures are composed by a large number of units, so its detailed representation can become impractical. Figure 15 Homogenization technique [19] Homogenization technique is used to derive the equivalent material properties and failure characteristics for solid brick masonry. Two approaches are possible: to obtain the average parameters from experimental tests, which can result expensive and the results are limited to the conditions of the experiments, or to derive the composite behavior from a representative volume element, which is out of the scope of this thesis. The properties needed for the analysis of a homogenized masonry wall can be taken from previous investigations [19]. Nevertheless, the studied homogenized wall is assumed to be composed of calcium silicate only. A further study about the influence of the mortar bonds is carried out in the following chapter. Homogenized models require a coarser mesh than micro or detailed models; hence numerical solutions are obtained easily. In spite of that, there is a limitation on the minimum element size for masonry elements: each element should contain some portion of masonry units and mortar, so that the size element cannot be chosen randomly because that could lead to an inappropriate post peak behavior [17]. In the case of concern, in which joints are not taken into account, the size of the element has no other restriction but numerical convergence. The scope of the study is to investigate the influences of the parameters that determine the configuration of a common masonry wall in its global behavior under out-of-plane solicitations. Studied parameters are the aspect ratio of the wall (ratio between height and length), the thickness of the wall, the vertical load level and the boundary conditions at four edges. The dimensions of the wall and boundary conditions studied are based on the most commonly values used in Germany. Analyses on the fracture mechanism, bearing capacity stress states along the experiments are done.
Numerical analysis of the out 4.1. Description of the model 4.1.1. Geometry The model is composed by a homogenized masonry wall of The wall is supported by concrete beams have a thickness of 0.5 study are shown. Figure 16 Geometry of walls A, E and I. Wall A has three fixed edges and the top free edge, Wall E is totally hin Two different materials are used in the model. The material “Concrete” is the constituent of the wall’s frame. For simplicity, concrete modulus equal to 32 GPa and Poisson’s ratio equal to 0.3. Concrete damaged plasticity material − Density: 2400 kg/m 3 − Elastic range: E=9e9 N/m − Plastic range: with dilation angle of 36° Table Compressive plastic behavior Stress (MPa) 1 0 20 0,1 When the boundary conditions are prescribed directly on the wall, singularities appear. The maximum stresses and strains are concentrated on the conditions are applied, leading In order to avoid this effect , shown in figure 17 Numerical analysis of the out -of- plane behavior of unreinforced masonry walls 34 of the model The model is composed by a homogenized masonry wall of length L, h eight H and thickness t. The wall is supported by concrete beams, in which the boundary conditions are applied. The a thickness of 0.5 m. In figure 16 the geometry of the three cases object of the Geometry of walls A, E and I. Wall A has three fixed edges and the top free edge, Wall E is totally hin ged and Wall I is totally fixed Two different materials are used in the model. The material “Concrete” is the constituent of For simplicity, concrete is assumed to behave only elastically with GPa and Poisson’s ratio equal to 0.3. Calcium silicate is material , with the following parameters: N/m 2 and v=0.12 with dilation angle of 36° Table 8 Material properties used in the wall models Compressive plastic behavior Tensile plastic behavior (MPa) Strain Stress (MPa ) Strain 0 2 0 0.0027 0,2 0.1 0.1 When the boundary conditions are prescribed directly on the wall, singularities appear. The strains are concentrated on the elements where leading to a wrong response of the mode l, in which the edges plastify , shown in figure 17 , a concrete frame is used. plane behavior of unreinforced masonry walls eight H and thickness t. boundary conditions are applied. The the geometry of the three cases object of the Geometry of walls A, E and I. Wall A has three fixed edges and the top free edge, Two different materials are used in the model. The material “Concrete” is the constituent of elastically with elastic is modeled by the When the boundary conditions are prescribed directly on the wall, singularities appear. The where the boundary l, in which the edges plastify .
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 35 Figure 17 Plastic strain distribution in absence of concrete frame 4.1.2. Contact Modeling The interaction between the elements involved in the model is defined by using a contact formulation provided by Abaqus. The interaction between bodies can be modeled by using two formulations: small-sliding, in which surfaces can undergo relatively small sliding but arbitrary rotation and finite-sliding, where separation and sliding of finite amplitude and arbitrary rotation of the surfaces are allowed. The small-sliding formulation is adopted. Possible contact conditions are defined by identifying and pairing potential contact surfaces, in which the contact elements are generated automatically. There are two surfaces in the sliding interface, the slave, covered by elements, and the master, defined as a slide line composed of a series of nodes. In Abaqus/Standard different contact models are available, among them, the implemented approaches for normal and tangential contact behaviors are explained next. 4.1.2.1. Tangential contact Two approaches were used initially for modeling the tangential contact between the wall and the concrete frame: penalty behavior and rough friction. Penalty Friction Penalty behavior is a stiffness method that permits some relative motion or elastic slip of the surfaces when they should be sticking. While the surfaces are sticking the magnitude of sliding is limited to this elastic slip. Abaqus continually adjusts the magnitude of the penalty constraint to enforce this condition. Contact between concrete and masonry is defined by an isotropic friction coefficient of 0.8, without a shear stress limit and a maximum elastic slip defined by the fraction of characteristic surface dimension of 0.005. Some problems emerge when this approach is used: the wall slips from the frames depending on the subjecting conditions. Due to the lack of confinement, the pressure normal to the surfaces is not large enough to ensure the necessary effective friction to prevent the wall from slipping. In order to avoid this effect, and instead of using horizontal pressure, the rough friction is chosen.
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 36 Rough friction In order to prevent the wall from loosing contact with the concrete frame, so that the boundary conditions can be correctly applied, the rough friction formulation is implemented. This formulation specifies an infinite coefficient of friction, in order to prevent the elements from slipping regardless of contact pressure. With this formulation, all relative sliding motion between two contacting surfaces is prevented as long as the corresponding normal direction contact constraints are active. In figure 18, deformed shapes of the wall are shown when frictional contact or rough contact friction models are used. Figure 18 Comparison of the deformed shape depending on the contact formulation used: tangential friction only (a) and rough friction (b) 4.1.2.2. Normal contact Both concrete and masonry are assumed to be impenetrable rigid bodies. This is modeled by the hard contact formulation, which is described next. Hard contact This model defines contact pressure between two surfaces at a point, p, as a function of the overclosure or interpenetration of the surfaces, h. The formulation of the contact is written as: Closed , 0 Open , 0 0ph 0hp ⇒>= ⇒ < = (25) Contact stiffness is, by default, assumed to have a linear behavior. In this model separation of contacting surfaces can be allowed or not. Convergence difficulties may arise if a closed contact interface with rough friction opens, so hard contact is typically used in conjunction with the no separation contact pressure-overclosure relationship. Despite of that, as separation between bodies can occur in reality, separation is allowed in the model.
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 37 4.1.4. Out-of-plane load Seismic design of masonry buildings can be carried out with different approaches, either dynamic time-history analysis or displacement-based quasi-static seismic analysis. In this chapter, unreinforced masonry walls are subjected to monotonic out-of-plane solicitations. For this purpose, it is appropriate to assume that failure of the wall is induced by out-of-plane acceleration. The maximum accelerations produce out-of-plane distributed inertia forces, so that in the model, a uniformly distributed out-of-plane pressure is applied in the wall. This pressure is increased linearly in each step of the analysis until the wall is forced to bend and fail. 4.2. Wall A The first group of walls object of this study are rectangular homogeneous calcium silicate walls with three fixed edges and one free edge. The top one is free, thus, without any restriction. Five different configurations are defined for the parametrical study. Variations on the aspect ratio (H/L), thickness of the wall and vertical load levels are undertaken, while a height of 2.4 m is maintained constant in all the cases. Table 9 Combination for the wall with top free edge H/L Thickne ss (m) Overpressure (MPa) A 0. 96 0. 24 0. 1 Aa 1. 92 0. 24 0. 1 Ab 0. 96 0. 175 0. 1 Ac 0. 96 0. 365 0. 1 Ap 0. 96 0. 24 0. 1 4.2.1. Results and discussion 4.2.1.1. Influence of aspect ratio of the wall The load-displacement response of the wall is compared for different values of aspect ratio. The horizontal load is calculated as a sum of reaction forces at the constrained nodes and the maximum displacement is reached by the middle point of the upper edge of the wall. As the analysis is force-controlled, when the compressed elements reach the yield stress, the reaction force becomes constant while the displacement would increase infinitely. Beyond this point, the numerical analysis is stopped. Figure 19 shows the results for cases Aa and Ac.
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 38 Figure 19 Influence of the aspect ratio As expected, the wall with a higher aspect ratio (Wall Ac with H/L=1.92), has a greater bearing capacity than the wall with a lower ratio (Wall Aa with H/L=0.96). The peak value of the reaction force is more than double for a double aspect ratio, while the maximum displacement of the most deflected point of the wall is similar. 4.2.1.2. Influence of thickness of the wall Like in the previous case, the load-displacement response of the wall is compared for the most typically used thicknesses of brick: 24 cm (Wall A), 17.5 cm (Wall Ab) and 36.5 cm (Wall Ac). Assuming that the wall is made by one layer of bricks, its thickness corresponds to the thickness of the brick. Results are shown in figure 20. Figure 20 Influence of thickness 0 2 4 6 8 10 12 0,00 0,02 0,04 0,06 0,08 0,10 Force F (MN) Max displacement d (m) Wall Aa Wall Ac 0 2 4 6 8 10 12 0 0,05 0,1 0,15 0,2 0,25 Force F (MN) Max displacement d (m) Wall A Wall Ac Wall Ab
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 45 The wall with a higher value of H/L (wall E with H/L=1.92), has initially a greater bearing capacity than the wall with a lower ratio (wall Ea with H/L=0.96). Nevertheless, both walls have a similar force-displacement response. Both of them reach the failure for the same maximum reaction force, while the maximum displacement measured at the midpoint of the wall is slightly greater for wall E. When the external force is 0.85 MN, the maximum force supported by the wall with lower aspect ratio is slightly greater than the reaction force of the other wall. Beyond that point, the reaction force is maintained constant while the maximum displacement increases from 5mm to 2.5 cm. In this case, the influence of aspect ratio has not the same effect on the behavior of the wall as in the walls A, studied before, so for more restricted boundary conditions, this parameter is not as influent on the resistance of the wall. 4.3.2.2.2. Influence of thickness of the brick Like in the previous study, three brick thicknesses are compared: 24 cm, 17.5 cm and 36.5 cm, which correspond respectively to walls E, Eb and Ec. The results can be seen in figure 30. Figure 30 Influence of thickness in wall E As observed in group A, the thickest wall (Ec) has the greatest bearing capacity, 1.95 MN, which is about 4 times greater than the bearing capacity of the wall with less thickness (0.55 MN) and about the double of the medium wall E (0.9 MN). As remarked before, the greater the thickness, the greater the bearing capacity and lower the flexibility of the wall. The deflection at failure of the different thicknesses is also remarkable. The wall with less thickness behaves in a more ductile way, so the maximum deformation reaches a value of 15 cm, while in the other walls the maximum deformation is 10 and 5 times lesser. This fact is related to the failure due to non-convergence of the model so that the strains are too great. After the elements that contribute to the resistance of the wall have plastified the experimental behavior is supposed to give a decaying force-displacement curve. As the 0 0,2 0,4 0,6 0,8 1 1,2 1,4 1,6 1,8 2 -0,01 0,01 0,03 0,05 0,07 0,09 0,11 0,13 0,15 Force F (MN) Max. displacement d (m) Wall E Wall Eb Wall Ec
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 46 numerical simulation is force-based, when this deformation is reached, the force becomes asymptotic. An important difference on the behavior of these walls with the walls of group A is how the bearing capacity is achieved. While walls of group E reach their bearing capacity with a low value of the maximum deformation, compared with the maximum deformation at total yield, walls of group A reach it while the deflections increase at a similar rate. 4.3.2.2.3. Failure mechanism Plastic strains in the non-loaded side, where the tensile stresses appear, follow in all cases diagonal lines, which appear initially in the corners of the wall and are connected in some point near the middle height of the wall. The failure mechanism varies depending on the aspect ratio. The wider is the wall, the longer is the horizontal line at the middle height. For the wall with lower aspect ratio, the diagonal lines join in the middle of the wall, and the horizontal line does not appear. The failure mechanism is shown in figure 31. Figure 31 Plastic strains at ultimate state in wall E at steps 7 and 14 This failure mechanism is contrasted with experimental tests results [21]. As noticed before, the material used is different and the assumptions made on the model can lead to different results, but the failure mechanism can be compared to the crack pattern produced in the experiments, which show that a wall with the same boundary conditions and slightly different dimensions cracks diagonally, with the cracks emanating from each corner towards the center (figure 32). More details of the test are given in the validation of the model (section 5.4). Figure 32 Two-way bending cracking pattern [6] The stress state at different stages of the analysis is now analyzed at the non-loaded side of the wall. Figure 33 (a) shows the spreading pattern of tensile stresses at an initial stage. The maximum tensile stresses are predominantly situated at the corners of the wall, as well as in its middle. In a more advanced step (figure 33 (b)) tensions are spread predominantly in vertical directions, which show where the tensile plastic strains will firstly appear.
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 47 Figure 33 Stress state at steps 5 (a) and 8 (b) In figure 34 the lasts stress states are shown. Tensile yield stress is reached along the vertical line remarked before, while compressive stresses keep increasing in the other side of the wall. Figure 34 Stress state at steps 11 (a) and 14 (b) The tensional state of the most stressed point, which is situated in the middle of the wall, is the first that reaches tension yield stress. As figure 35 shows, plastic strains increase beyond this state is reached while stresses do not increase. The surrounding points develop a similar behavior, so that plastic strains are spread and the fracture mechanism is formed. Figure 35 Stress-plastic strain in the most tensed point -0,5 0 0,5 1 1,5 2 2,5 0 0,001 0,002 0,003 0,004 Stress S22, (MPa) Plastic strain
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 48 4.3.3. Wall I Walls of group I are a set of models in which the boundary conditions in the four edges are fixed. That means that rotation and displacements are constrained in all directions. Four different configurations are compared as in the previous cases (table 11). 4.3.3.1. Combination Table 11 Combination of walls for BC I H/L Thickness (m) Pre compression (MPa ) I 0,96 0,24 0, 1 Ia 1,92 0,24 0, 1 Ib 0,9 6 0,175 0, 1 Ic 0,96 0,365 0, 1 4.3.3.2. Results Force-displacement curves, stress states and plastic strains are studied for the different configurations. 4.3.3.2.1. Influence of aspect ratio of the wall Influence of aspect ratio in the behavior of the wall is studied by the results obtained and shown in figure 36. Figure 36 Influence of the aspect ratio in wall I The wall with a higher aspect ratio (Ia with H/L=1.9) has a greater bearing capacity (maximum force supported by the wall) (23 MN) than wall I, with a lower ratio H/L=0.9 (14 MN). The 0 5 10 15 20 25 0 0,01 0,02 0,03 0,04 0,05 Force F (MN) Max. displacement d (m) Wall I Wall Ia
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 49 maximum displacement, measured at the midpoint of the wall, in which the wall is completely yielded, is comparably greater for the wider wall. While the wider wall deflects up to 4.5 cm the other deflects less than 2.5 cm. As expected, a narrower wall can resist a greater out-of- plane pressure. 4.3.3.2.2. Influence of thickness of the brick In figure 36 the influence of changes in the thickness of the wall is studied. Figure 37 Influence of thickness in wall I The thickest wall (Ic) has the greatest bearing capacity, 30 MN, which is about the triple value than the bearing capacity of the wall with less thickness (10 MN) and more than the double of the medium wall E (15 MN). As in the cases studied before, the greater the thickness, the greater the bearing capacity and lower the flexibility of the wall. The deflection at failure of the different thicknesses is also remarkable. The wall with less thickness behaves more flexibly, so the maximum deformation reaches a value of 14 cm, while in the other walls the maximum deformation is 7 and 4 times lesser. 4.3.3.2.3. Failure mechanism The failure mechanism for the totally fixed wall is similar to the failure mechanism obtained in the hinged wall. By observing the direction of the maximum plastic strains in the non-loaded side (figure 38), the mechanism of failure is derived. Once again, the maximum plastic strains follow in all the cases diagonal lines; nevertheless, they appear initially on the edges of the wall, where the boundary conditions are transmitted by the frame (figure 38 a). Once the edges of the wall have plastified, the stresses are concentrated on the centre of the wall; 0 5 10 15 20 25 30 0 0,02 0,04 0,06 0,08 0,1 0,12 0,14 0,16 Force F (MN) Max. displacement d (m) Wall I Wall Ib Wall Ic
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 50 hence the fracture lines are propagated from the central point to the corners, following diagonal lines. Figure 38 Plastic strains at initial state (a) and ultimate state (b) on wall I The failure mechanism slightly differs depending on the aspect ratio. It is observed that the wider is the wall in relation to the height, the more homogeneously are propagated the yield lines to the corners. For the wall with lower aspect ratio, a vertical line of yielded elements initially appears. Figures 39 to 41 show the stress in the Y direction (horizontal direction) of the loaded side of the wall at different steps of the analysis. Figure 39 Stress states at steps 1 (a) and 8 (b) In the initial steps (figure 39) the external load mainly creates compressive stresses in the middle part of the wall, while some tensile stresses appear on the middle of its upper edge. Figure 40 Stress state at steps 15 (a) and 20 (b)
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 51 In a more advanced state of the analysis, a smaller area situated in the middle of the wall is committed to bear the compressive stresses produced by the out-of-plane load, while the tensile stresses keep increasing in the lower and upper edges. At this stage, tensile stresses almost reach yield stress, so plastic strains start to form. Figure 41 Stress state at steps 25 (a) and 34 (b) In a final stage of the analysis, represented in figure 41, tensile yield stress is spread along the four edges, while the compressed part begins to plastify. At failure (figure 41 b), yield compressive stresses are propagated in the surrounding points predominantly following horizontal direction. Moreover, stress-plastic strain state developed in the point situated in the middle of the wall, which is subjected to the greatest strains and stresses, is represented on figures 42 and 43. On one hand, the point situated on the compressed side develops plastic strains when a compressive stress of 15 MPa is reached, so that compressive yielding is not achieved. Beyond this point, stresses increase, as well as plastic strain do, until yielding is overcome. Figure 42 Stress-plastic strain curve in the most compressed point of wall On the other hand, the stress-plastic strain state at the opposite side of the wall, is subjected to tensile stresses, so that plastic strains approximately appear for stresses about 2 MPa. Beyond the tensile yield stress, plastic strains increase but not stresses. -35 -30 -25 -20 -15 -10 -5 0 -0,005 -0,004 -0,003 -0,002 -0,001 0 Stress S22 (MPa) Plastic strain
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 52 Figure 43 Stress - Plastic strain curve in the most tensed point 4.3.4. Overall comparison: influence of the boundary conditions In Figure 44, the influence of the boundary conditions is analyzed for each of the previously studied cases with dimensions of table 12. Table 12 Wall properties for the influence of boundary conditions H/L Thickness (m) Pre compression (MPa ) 0. 96 0. 24 0. 1 As a reminder, wall A has three fixed edges and the upper edge free, wall I is totally fixed and wall E is totally hinged. Figure 44 Influence of the boundary conditions -0,5 0 0,5 1 1,5 2 2,5 0 0,002 0,004 0,006 0,008 0,01 0,012 0,014 Stress S22 (MPa) Plastic strain 0 2000000 4000000 6000000 8000000 10000000 12000000 14000000 16000000 0 0,02 0,04 0,06 0,08 0,1 0,12 0,14 0,16 0,18 0,2 Force F (N) Max. displacement d (m) Wall A Wall E Wall I
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 53 Different boundary conditions lead to notably different load-displacement response. The fewer degrees of freedom has the wall, the greater bearing capacity is expected. Totally fixed boundary conditions lead to a peak value of the force of 14 MN, reached for a maximum displacement of 4cm. Wall A, fixed and with a free edge, has a bearing capacity of almost 3 MN, while wall E, which their edges are hinged, of 0.3 MN. It is worth to notice that fixed boundary conditions increase considerably the bearing capacity, as well as that the flexibility of the wall is reduced. 4.4. Conclusions Although the model used for the acquisition of these results is a homogenized model and the influence of the mortar is not taken into account, it is sensible to compare different results because they are obtained by taking the same assumptions. The most important assumption is that the wall acts as a uniform slab, which does not take into account the presence of joints, and thus, the weak lines of failure. The walls fail when the material is plastified and reaches the yield tensions in some points, which are assumed to be the failure lines. It is worth to notice that the same model can be improved by considering the presence of mortar and by validating it with experimental results. • Vertical load level: although for the pre-compression levels studied a significant difference between the results cannot be appreciated, a greater compression must lead to a greater bearing capacity of the structure. This is explained by the confinement caused by a vertical pressure when the vertical edges of the wall are constrained on the orthogonal direction. As experimental experiences suggest, it is expected a major difference between the results. The assumptions made on the model may lead to homogenize the response of the walls under different values of vertical load levels. • Aspect ratio: the influence of this parameter is significant. It has been observed that the greater the parameter H/L is, the greater the resistance of the wall. Thus, it is recommended to construct narrower walls, or in the cases, in which it is not possible, create the appropriate load path, by using columns or I-shaped beams. • Boundary conditions: as fixed boundary conditions lead to a greater bearing capacity, this option is recommended. • Thickness: it is observed that the thicker the wall is, the greater is its bearing capacity but lesser its deflection at failure. Thus, it is preferable to use thicker bricks.
Numerical analysis of the out 4.5. Different meshing sch A convergence test on the influence of element size is done in order to study computational accuracy of the model. Three different meshes are them using eightnode linear hexahedral solid elements of type C3D8R Table 13 Characteristics of the mesh Coarse mesh Medium mesh Fine mesh Figure 45 Coarse, medium and fine The results obtained for a wall under the same subjecting and loading conditions and the meshes shown above are compared in terms of the for Moreover, the committed error on the numeri model is behaving in the face of refinement of the mesh. Figure 46 Comparison of the results for meshes shown in figure 4 0 100000 200000 300000 400000 500000 600000 700000 800000 900000 1000000 0 0,005 Force, F (N) Numerical analysis of the out -of- plane behavior of unreinforced masonry walls 54 Different meshing sch emes A convergence test on the influence of element size is done in order to study computational accuracy of the model. Three different meshes are tested node linear hexahedral solid elements of type C3D8R . Characteristics of the mesh used in the study of convergence Number of elements Number of nodes Coarse mesh 1 648 912 mesh 4800 3222 9647 7152 Coarse, medium and fine meshes used in the convergence test The results obtained for a wall under the same subjecting and loading conditions and the meshes shown above are compared in terms of the for cedisplacement curve (figure 46 Moreover, the committed error on the numeri cal analysis is calculated in order to see how in the face of refinement of the mesh. Comparison of the results for meshes shown in figure 4 5 0,005 0,01 0,015 0,02 0,025 0,03 Max. displacement, d (m) plane behavior of unreinforced masonry walls A convergence test on the influence of element size is done in order to study the (figure 45); all of meshes used in the convergence test The results obtained for a wall under the same subjecting and loading conditions and the displacement curve (figure 46 ). cal analysis is calculated in order to see how the 0,035 0,04 Medium mesh Fine mesh Coarse mesh
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 61 Uncoupled traction-separation behavior is used, thus, the stiffness coefficients are defined in each direction by using the data of table 15. Table 15 Stiffness coefficients Stiffness coefficients K nn 3 MPa/m m K tt =K ss 1 MPa/m m These values of stiffness are derived from the maximum values of traction in each direction, which correspond to the cohesion in both t and s directions and tensile strength in the normal direction of the surface. For mortar, tensile strength is assumed to be 0.1 MPa. Cohesion damage The degradation of failure of the bond is simulated by means of a damage initiation criterion and a damage evolution law. When the damage evolution law is not specified, the damage initiation criterion is evaluated for output purposes only. Figure 50 Typical traction-separation response in the cohesive model [14] The beginning of the degradation of the cohesive response is assumed to happen when the maximum stress criterion is accomplished: 1,,max 000 = t t s s n n t t t t t t (37) where the peak values of the contact stress are taken as t 0 n =0.1 MPa, t 0 s =1.8 MPa and t 0 t =1.8 MPa. Apart from the formulations of the damage and the damage initiation criterion used, there are other options.
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 62 5.1.2. Numerical simulations 5.1.2.1. Two-bricks shear test In a first approach, cohesive behavior is not taken into account and three contact models are compared. The hard pressure-overclosure normal contact is combined with three tangential formulations: uniform tangential frictional model with μ=0.8, a frictional model with slipdependent friction coefficient (with data specified in table 14) and a slip rate dependent frictional model in which a tangential stress limit is defined. The analysis is made by means of a simulation of the simple shear test in which two bricks are joined by their biggest face, and the brick on the top is pushed on its axial direction while the other one is fixed on its lower face. As in the experimental test, a normal compression of 0.1 MPa is applied in the top face of the upper brick. The effect of the contact modeling is studied by means of the force-relative displacement curve, which is shown in figure 52. The force is calculated as the sum of the reaction forces in the horizontal (axial) direction on the nodes of the subjected face, and the displacement is measured on the upper brick. Figure 51 Influence of the contact formulation in the simple shear test While in the isotropic frictional model the bricks slide from the beginning of the analysis without frictional resistance, the model with slip-dependent rate data seems to have initially a greater frictional resistance. The purpose is to simulate a cohesive behavior by giving a large coefficient of friction for a slip-rate equal to 0 (no differential slip occurs) followed by the real coefficient of friction for positive slip velocities. Nevertheless, for numerical reasons, a smooth coefficient of friction – slip rate curve must be described, so the real behavior cannot be achieved by this description. The results when a tangential tension limit is specified show that the analysis is stopped when this tangential stress is reached in some points. When this value 0 5 10 15 20 25 0,0E+00 5,0E-05 1,0E-04 1,5E-04 2,0E-04 2,5E-04 3,0E-04 3,5E-04 4,0E-04 Force (kN) Relative displacement (m) Friction 0.8 Slip-Rate Initial=150 Slip Rate + Limit tang
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 63 is reached, the surfaces should slide freely, as if the coefficient of friction was equal to zero. Summarizing, the action of mortar cannot be precisely defined only by using hard and frictional models, so cohesive properties must be implemented. Cohesive contact properties are added to the model without defining a damage law. The same analysis is carried out, so that shear-relative displacement relationship is obtained. Moreover, a traction test is also done with the purpose of obtaining the traction–relative displacement curve (figure 52 b). On the other hand, the normal hard contact relationship is modified in order to allow the surfaces to transmit tensile contact pressures up to a value of 0.1MPa before they separate. If this pressure is exceeded at a node, the status of the contact is changed. This contact option is useful where negative pressure values (surface cohesion) may be allowed physically and also, to overcome numerical problems in difficult contact simulations and to avoid excessive iterations. Figure 52 Shear-relative displacement and traction-separation displacement response of the model In one hand, the shear-displacement relationship shows a shear limit beyond which relative displacement in the tangential directions is allowed. If the shear stress is lower than this value, relative movement is not produced. That limit is due to the cohesion of the Coulomb’s frictional model. As the shear-relative displacement depends on the normal compression applied to the bricks, it is difficult to compare to the available experimental tests. In the other hand, the traction-separation curve shows the traction forces induced while one brick is separated from the fixed one in the normal direction of the surfaces in contact. As expected, the relative displacement is nearly zero until the tensile strength is overcome. Beyond this point, displacements increases while the traction decreases and for further displacements, there is no opposition to movement. 5.1.2.2. Contact study with a wall sample The study of the contact is now extended to a wall sample, constituted by ten brick layers and a width corresponding to two bricks. The analysis consists on a simply supported wall 0 2 4 6 8 10 12 14 16 18 -0,001 0,001 0,003 0,005 Shear strenght(MPa) Rel. Displacement d (m) -20 0 20 40 60 80 100 120 140 160 0 0,000005 0,00001 traction t (Pa) Rel. Displacement d (m)
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 64 subjected to out-of-plane pressure, under a vertical load of 0.1 MPa. The size of the calcium silicate bricks is 0.23x0.07x0.11 m 3 and the contact formulations used are mentioned. Two contact models are compared. A model with contact defined only by penalty frictional behavior and hard normal contact is compared to the same model with cohesive contact added. The load-displacement response of the model and the stress state at the moment in which the peak value is achieved is compared to the same results of a model in which cohesive contact is included. The values used for contact modeling are the same as in the previous chapter. Figure 53 Influence of cohesion between bricks on the wall sample The cohesive model has a slightly higher bearing capacity (0.32 MN and 0.34 MN) than the only frictional one. Even though, this peak value is reached for a higher (approximately, the double) mid displacement, what means that if the contact has cohesive properties, what is more realistic, the wall can resist greater maximum deformations. 0 0,05 0,1 0,15 0,2 0,25 0,3 0,35 0,4 0 0,002 0,004 0,006 0,008 0,01 0,012 0,014 Force, F (MN) Displacement, d (m) Cohesive contact No cohesive contact Slip - dependent friction
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 65 Tangential frictional and hard normal contact In figure 54 the stress state of the wall is shown as a contour in the deformed shape. The last image shows the maximum principal plastic strains. Figure 54 Stress states and plastic strains in the wall sample without cohesion Since the plastic strains are concentrated on the nodes in which fixed boundary conditions are applied, and the bricks situated in the most deflected part are losing their contact, the wall fails due to the weakness of mortar. The numerical analysis does not calculate beyond the point in which the separation between bricks is too large, so that not enough nodes of the slave surface are in contact with the master surface. Tangential frictional, hard normal and cohesive contact As before, the stress state of the wall is shown as a contour in the deformed shape (Figure 55) when cohesion is taken into account. The last image shows the maximum principal plastic strain. Figure 55 Stress states and plastic strains in the wall sample with cohesion As in the latter case, the bricks in the most deflected part of the wall are losing their contact, and the wall fails due to the weakness of mortar. The numerical analysis does not calculate beyond the point in which the separation between bricks is too large. A study of the different contact formulations is done. Since the behavior of the wall is more appropriate when using this formulation, for the detailed masonry wall, the cohesive contact behavior should be added to hard normal contact and penalty tangential formulations.
Numerical analysis of the out 5.2. Numeric al model of a detailed UMW under A detailed masonry wall with the same geometrical homogenized model is studied Figure Moreover, the contact between bricks is described by using a contact formulation between surfaces. The model of the contact properties is studied in model, with penalty friction tangential model is implement 5.2.1. Numerical results and discussion H/L L (m) A 1. 9 2. 5 Aa 0. 9 1. 25 Ab 1 . 9 2. 5 Ap 1. 9 2. 5 I 1. 9 2. 5 5.2.1.1 Non cohesive model A non cohesive model is developed isotropic friction c oefficient of 0.8. The model is v horizontal confinement pressure mm on each side in order to make th directions effective. Numerical analysis of the out -of- plane behavior of unreinforced masonry walls 66 al model of a detailed UMW under monotonic out- of - A detailed masonry wall with the same geometrical and material properties homogenized model is studied . Figure 56 Numerical model of the detailed masonry wall Moreover, the contact between bricks is described by using a contact formulation between surfaces. The model of the contact properties is studied in section 5.1 . A hard normal contact model, with penalty friction tangential model is implement ed. Numerical results and discussion Table 16 Combinations of the detailed model (m) t (m) Boundary Conditions Compression (MPa) 0. 24 Fixed and free on top 0.1 25 0. 24 Fixed and free on top 0.1 0.1 75 Fixed and free on top 0.1 0. 24 Fixed and free on top 1.0 0. 24 Four edges fixed 0.1 5.2.1.1 Non cohesive model developed in which contact between bricks is modeled only by a oefficient of 0.8. The model is v ery dependent on the over horizontal confinement pressure is int roduced by means of an imposed displacement of in order to make th e frictional contact in both vertical and horizontal plane behavior of unreinforced masonry walls of - plane loading (figure 56) as the Moreover, the contact between bricks is described by using a contact formulation between . A hard normal contact Compression (MPa) 0.1 0.1 0.1 1.0 0.1 in which contact between bricks is modeled only by a ery dependent on the over -pressure and a roduced by means of an imposed displacement of 0.1 e frictional contact in both vertical and horizontal
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 67 Influence of the aspect ratio of the wall Following the same procedure as in the homogenized wall, an analysis about the influence of the aspect ratio, as well as other parameters, is carried out. The force-maximum displacement curves obtained with the numerical model until failure of the wall (reached when the failure mechanism is formed, thus, yield is performed in several elements and plastic strain become too large to continue with the calculations) are compared for each value of the parameters. Figure 57 Influence of the aspect ratio in the detailed model As expected, the wall with a greater aspect ratio, A, has a lower bearing capacity than wall Aa. In this case, the wall Aa fails when the out-of-plane force reaches 5.5 MN, while the wall A fails at 3.2 MN. Both of them can resist a similar maximum displacement, between 4 and 6 cm. Influence of the thickness of the wall Figure 58 Influence of the thickness of the wall in the detailed model 0 1 2 3 4 5 6 0 0,02 0,04 0,06 0,08 Force F (MN) Displacement d (m) A Aa 0 0,5 1 1,5 2 2,5 3 3,5 0 0,02 0,04 0,06 0,08 0,1 0,12 0,14 Force F (N) Displacement d (m) A Ab
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 68 As happened in the homogenized model, it is shown (figure 58) that walls with higher thickness have greater bearing capacity. Wall A, with a thickness of 24 cm, is able to bear 3.25 MN, while wall Ab, with 17.5 cm of thickness, just 2.2 MN. It is also remarkable that the thin wall is more flexible, so yields at a double maximum displacement, which is measured at the highest point of the wall. Influence of the vertical load level of the wall Two different vertical load levels are tested. Pressures of 0.1 MPa and 1 MPa are applied to the free edge of wall A. Figure 59 Influence of the vertical load level in the detailed model It is worth to notice that the bearing capacity of the wall with a higher vertical compression is greater than in the wall subjected only to 0.1 MPa of vertical load. Walls with higher verticalpre compression are expected to perform greater strength capacity, and, in particular, postpeak strength capacity. That is caused by the increased flexural and frictional resistance of the bed joints in the post-cracked state, due to the higher axial stress [12]. Even though, as well as in the homogenized model, this increment on the bearing capacity is low. While under a compression of 1 MPa, the peak load is 1.75 MN, under 0.1 MPa, the wall can resist up to 1.5 MN. Influence of the boundary conditions The behavior of the wall with all its boundary conditions fixed is compared previous one. The bearing capacities of the walls as well as their fracture mechanisms are analyzed. 0 0,2 0,4 0,6 0,8 1 1,2 1,4 1,6 1,8 2 -0,02 0 0,02 0,04 0,06 0,08 0,1 0,12 0,14 0,16 0,18 Force F (MN) Displacement d(m) p=0.1MPa p=1MPa
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 69 Figure 60 Influence of the boundary conditions of the detailed wall In figure 60 it is observed that the most restricted wall with all its edges fixed has a greater resistance for the same maximum displacement. This fact also happened in the homogenized model. For wall I, displacements are measured at central node. While the fixed wall has a bearing capacity of 4.5 MN, wall A, with the top free edge, resists 3 MN. Even though, for low out-of-plane loadings, the behavior is similar. Failure mechanism and stress states of wall A Figure 61 shows the stress states of the wall with the top free edge at two stages of the analysis. The second picture corresponds to the last step, where yield tensile stresses are reached in the upper part of the wall. It can be seen how the bricks are losing their contact. Figure 61 Stress states of the detailed model A at steps 7 and 9 Figure 62 shows the stress and plastic strains relationship for the most compressed point of the wall, which corresponds to the middle point in the upper edge of the compressed side. In 0 0,5 1 1,5 2 2,5 3 3,5 4 4,5 5 0 0,01 0,02 0,03 0,04 0,05 0,06 Force F (MN) Displacement d (m) A I
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 70 this point, plastic strains appear for a compressive stress in the Y direction, which is perpendicular to the out-of-plane load, equal to 3.5 MPa. Beyond this point, compressive stress increases approximately linearly with plastic strains up to a value equal to the compressive yield stress (20 MPa), reached for a plastic strain equal to 0.0014. At this point, the numerical analysis is stopped. Figure 62 Stress- Plastic strain in the most compressed point By observing the maximum plastic strains evolution, shown in figures 63, fracture mechanism can be completely defined. In the moment in which plastic strains appear, bricks begin to yield, so cracks appear. The fracture mechanism is a combination of failure in the mortar joints, acting as a plane of failure and leading to openings in the model, and formation of vertical cracks in the middle of the upper bricks. Figure 63 Plastic strains of wall A at different steps: when they appear, at their maximum value and at the last step of the analysis In the case of wall Aa with a lower aspect ratio, the fracture mechanism differs from the rest of the configurations. Tension is concentrated near the edges, so that the plastification is produced in two parallel lines situated near the fixed vertical edges. As can be seen from Figure 64 a, which represents the stress versus plastic strain in the most compressed point (situated in the middle of the upper edge), yield is not reached, even though plastic strains appear. Contrarily, yield is reached near the edges, and plastics strains at last step are shown in figure 64 b. 0 5 10 15 20 25 0 0,0005 0,001 0,0015 Stress s22 (MPa) Plastic strains
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 77 Comparison of the results In figure 72, results are compared in terms of reaction force – displacement on the middle height of the wall relationship. Figure 72 Comparison between experimental and numerical results The two main differences between experimental and numerical results, apart from peak resistance value, are that post-peak behavior can be described for the experimental test (and not for the numerical test, which is force-based) and that the experimental curve can be expressed in terms of a bi-linear curve, while the numerical result is clearly non linear. The latter is a consequence of the material model used, in which plastic behavior, or softening, is allowed. In reality, the material has a high degree of brittleness, so resistant strength is lost rapidly once cracks are formed. As it is obvious, the bearing capacity of the numerical model, as well as the deformation reached at ultimate strength, is much greater than in reality. Several parameters in the numerical model must be more appropriately defined. It is remarkable to notice that the presence of holes on the bricks is not considered in the model. This fact is supposed to have a great influence on the behavior of the wall. Other parameters that should be revised are the boundary conditions, which may not be applied in the same way as in the experimental test, in which there are return walls on both sides, and contact between bricks is considered frictional, due to the lack of information, among other reasons. Due to the slenderness of the wall and the plastic properties of the material model, the fracture mechanism differs from the real one. Figure 73 a shows the deformed shape (with a magnification in the out-of-plane direction of 40 times) and figure 73 b, the plastic strains. As can be seen, plastic strains are developed near the edges, when they are expected to appear in 0 10 20 30 40 50 60 70 80 90 0 0,005 0,01 0,015 0,02 0,025 0,03 Force F (kN) Mid-wall displacement, d (m) Experimental test Numerical analysis
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 78 the middle upper part of the wall, as happens in wall A, studied previously in this chapter (see figure 61). Figure 73 Deformation in the out-of plane direction (a) and plastic strains (b) Despite of that, this verification has been carried out in order to notice the significance of a model validation procedure, which due to the lack of the most convenient experimental test is not properly performed. 5.5. Unreinforced Masonry Wall under quasi-static cyclic out-of-plane loading The aim of this section is to investigate the seismic response of out-of-plane walls by means of an analysis of the wall under quasi-static cyclic loading. A hysteresis model, a numerical representation of the load-displacement relationship, is developed. A time history analysis to simulate the dynamic nonlinear response of the wall is made. It is not the aim to determine the seismic resistance to a particular earthquake. As in the static case, a parametrical study is performed. Variations on the aspect ratio and vertical load level are studied. Similar simulations can be performed in order to have representative data about the out-of-plane cyclic behavior of single walls. These data can become one of the sources of simulated results that are required in the displacement based design for masonry buildings. Moreover, data can be generated to make predictions about the resistance of the wall under more realistic earthquakes. Displacement based design for masonry buildings Displacement based design is based on the capacity spectrum method, developed by Freeman [23], which is a nonlinear static method that compares the seismic actions to the loading capacity of the building, taking the material behavior with its post-peak capacity into account. The building capacity is described by an inelastic cyclic pushover curve, and the seismic load is represented by the response spectrum. The intersection point between the curves transferred in the spectral acceleration – spectral displacement plane, is the “performance point”, which indicates the maximum spectral displacement for the spectrum [24].
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 79 In the displacement based design for masonry buildings, the cyclic load displacement curves (capacity curves) of single shear walls are used to determine the nonlinear push-over of an entire structure. The capacity curves of single walls are derived from interpolations of capacity and damping curves at different load levels and aspect ratios. These curves can be obtained by experimental tests, numerical simulations and analytical computation. The transformation of the curves into the Sa-Sd plane is based on a model of an equivalent single degree of freedom system. The influence of energy dissipation within the nonlinear range of the capacity curve is considered by a reduction of the linear elastic response spectrum by means of an effective viscous damping, which is the sum of the viscous damping and the equivalent viscous damping due to hysteretic behavior. Figure 74 Calculation of the equivalent viscous damping [25] and determination of the "Performance Point" In the case of concern, the results are evaluated from the force-displacement hysteretic response of the model under cyclic out-of-plane loading. The analyzed parameters, which are crucial for the displacement-based design, are described below: • Cyclic stiffness is defined as the slope of the line joining the origin and the peak value of the respective cycle. Propagation of cracks during cyclic loading causes the stiffness degradation in the specimen. The stiffness degradation of every cycle is the ratio between the stiffness at a particular cycle with respect to the first one [26]. • The energy dissipation is the area enclosed by load-deflection hysteresis curve and the energy input is the sum of energy dissipation and the restorable elastic energy: DEL EEE += (38) where E L is the total energy input, E E is the restorable elastic energy and E D is the dissipated energy. The specimen is capable of absorbing energy through plastic deformation. As the structures with higher energy dissipation capacity are safer for earthquakes, it is important to know their energy dissipation capacity in order to determine their seismic resistance. • The viscous damping ratio is calculated by the method of energy dissipated per cycle of loading, using hysteresis loops in the cyclic loading tests, as is described in figure 74.
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 80 Detailed unreinforced masonry wall under cyclic out-of-plane loading As well as in the static analysis, the behaviors of various unreinforced masonry walls are compared. The response of the detailed wall modeled without cohesion, only friction, subjected to different boundary conditions is studied. In order to determine the cycles, the pick load in each cycle is incremented linearly until a pressure that led to its ultimate resistance in the static analysis, by assuming a total of 7 complete cycles. The load history with variable amplitude is shown in figure 75. The maximum pressure resisted by the studied walls A and I under monotonic load is about 0.7 MPa. This value is taken as a reference to determine the cycles, which reach the 0.66 MPa in the last cycle. The behaviors of Wall A, Aa, Ab and I are compared. Figure 75 Out-of-plane loading history in the cyclic test for wall A It is expectable that walls dissipate a significant amount of energy through hysteresis loops. This is likely to be caused by the frictional resistance mechanisms, resulting in highly nonlinear and inelastic behavior. Good energy dissipation characteristics under cyclic loading are highly beneficial to the seismic performance of the structural system [27, 38]. Wall A The detailed wall with three fixed edges and free top edge studied in section 5.2 is now subjected to the previously defined cyclic out-of-plane pressure (figure 75). The response of the wall in terms of the hysteretic force-displacement is shown in figure 76. -0,8 -0,6 -0,4 -0,2 0 0,2 0,4 0,6 0,8 0 2 4 6 8 10 12 14 16 Horizontal Pressure (MPa) Time (steps)
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 81 Figure 76 Hysteretic response of wall A under cyclic test The wall can only bear up to a pressure of 588 MPa, that means that not all the cycles are completed. On the last cycle, the wall fails and the displacement increases until a value of 5 cm. Moreover, the force displacement response is not symmetric with respect the initial state of deformation; while for positive displacements (because these correspond to the first direction of the cycle) the maximum reaction force is 2 MN, for negative displacements and the same cycle the wall bears almost 3 MN. That effect may be due to the loss of energy dissipation capacity produced by the damage, which produces a permanent loss of deformation recuperation. Figure 77 Stress - Plastic strain developed in the most solicited point of wall A subjected to cyclic test -4 -3 -2 -1 0 1 2 3 -0,06 -0,05 -0,04 -0,03 -0,02 -0,01 0 0,01 0,02 Force F (MN) Displacement, d (m) -25 -20 -15 -10 -5 0 0 0,0005 0,001 0,0015 0,002 Stress S22, (MPa) Plastic Strain
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 82 In figure 77, the evolution of stresses in the Y-direction, perpendicular to the out-of-plane load, is plotted against plastic strains. The graph corresponds to the most stressed point, which is situated in the middle of the upper free edge. In this point, the plastic strains are initiated, and the stress increases until the compressive yield value (20 MPa). Wall I The detailed model of the wall subjected to fixed edges is submitted to the previous out-of- plane cyclic loading. In figure 78, the hysteretic force-displacement curve is shown. For the first cycles, the stiffness degradation cannot be appreciated, but as much as the peak value in each cycle increases, the stiffness degradation also does. That leads to energy dissipation, which corresponds to the area enclosed by the hysteretic response of the wall. Figure 78 Force-displacement response of the wall under out-of-plane cyclic load Figure 79 shows the stress – plastic strain relationship developed during the cyclic test in two points, situated in the two sides at the middle point of the wall. Point A corresponds to the side which is initially, for the first load increment, in compression. It can be seen that this point reaches compressive yield stress, and it behaves elastically. When a stress of 10 MPa is reached, this side of the wall behaves plastically, so that plastic strains appear. -4,1 -3,1 -2,1 -1,1 -0,1 0,9 1,9 2,9 3,9 Force F (MN) Displacement d (m)
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 83 Figure 79 Stress - Plastic strain of most solicited point of wall I subjected to cyclic loading Wall Aa The influence of the aspect ratio in the results of the cyclic test is studied by means of the comparison between the hysteretic curve of walls A and Aa. As remarked in the results of wall Aa under monotonic out-of-plane load, these walls behave differently. While wall A has the expected failure mechanism, wall Aa develops two vertical cracks near the edges. This phenomenon appears also under cyclic loading and may lead to a hysteretic forcedisplacement curve notably different to the corresponding to wall A. Figure 80 Hysteretic response of wall Aa under cyclic test Wall Aa completes only two of the cycles imposed until failure. As shown in figure 81, the stress achieved at the last step by the point situated in the middle of the upper edge of the wall is lower than the yield compressive stress. While wall A develops a bearing capacity -20 -18 -16 -14 -12 -10 -8 -6 -4 -2 0 -0,0071 -0,0061 -0,0051 -0,0041 -0,0031 -0,0021 -0,0011 -0,0001 Stress S22 (MPa) Plastic strain Middle point A Middle point B -3 -2 -1 0 1 2 3 4 -0,0025 -0,002 -0,0015 -0,001 -0,0005 0 0,0005 0,001 0,0015 0,002 0,0025 Force F(MN) Displacement
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 84 similar to the corresponding to wall Aa. Even though, as expected, the wall with higher aspect ratio reaches lower maximum deflection at these points, as less flexible that it is. The difference between maximum displacements is the 10%, so that, wall Aa deflects until a maximum value of 0.02, while wall A only reaches 0.002. Figure 81 Stress - Plastic strain in the most solicited point of wall Aa under cyclic test Wall Ab The influence of the thickness in the results of the cyclic test is studied by means of the comparison between the hysteretic curve of walls A and Ab. As in under monotonic load, wall Ab, which bricks have a thickness of 17.5 cm, behaves in a more ductile way, and has a lower bearing capacity than wall A, with a thickness of 24 cm. The differences in the behavior can be appreciated in the hysteric force-displacement, which is shown in figure 82. Wall Ab under cyclic loading, resists up to 2 MN for positive displacement and has a slightly lower bearing capacity in the opposite direction, where it fails. Figure 82 Hysteretic response of wall Ab under cyclic test -3,5 -3 -2,5 -2 -1,5 -1 -0,5 0 -0,0003 -0,00025 -0,0002 -0,00015 -0,0001 -0,00005 0 Stress S22, (MPa) Plastic strain -2,5 -2 -1,5 -1 -0,5 0 0,5 1 1,5 2 2,5 -0,15 -0,1 -0,05 0 0,05 0,1 Force F (MN) Displacement d (m)
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 85 Wall A has a similar bearing capacity for positive displacements, but contrarily, when it is subjected to an out-of-plane pressure with opposite sign, has a greater resistance (3 MN). Beyond that point, which is reached for a displacement of 2 cm, the wall fails. The maximum bearing capacity for wall Ab, which is expected to behave in a more ductile way, is reached when the most deflected point has a displacement of 5cm, and fails at a maximum displacement greater than 10 cm. Figure 83 Stress evolution developed in the most solicited point of wall Ab The failure mechanism of wall Ab coincides with the failure mechanism of wall A, which is explained above. Figure 83 shows the increasing values of the stresses in the most solicited point of the wall. It is noticed that the point experiments only compression stresses, so that it fails plastically due to crushing (or compressive yield). Even though, in the last cycle the yield compression stress is not fully reached. The reason why tensile stresses do not appear is that when bricks are subjected to tensile tresses, they tend to separate and normal contact is lost. At this point, contact pressure is zero and opening occurs. Conclusion Under seismic load, a structure is subjected to multiple reversed cyclic accelerations of increasing magnitude up to the peak ground acceleration and the structure exhibits corresponding levels of damage until reaching the peak displacement cycle [29]. Walls exhibit highly nonlinear and inelastic load-displacement behavior as shown by the hysteresis curves. Nonlinearities are caused by the frictional resistance mechanisms along crack lines and by rigid-body rocking mechanisms [1]. Moreover, walls undergo strength and stiffness degradation during the course of testing due to cumulative cracking [30]. In reality, the overall degradation results from several irreversible types of damage, including progressive tensile and shear cracking of the brick-mortar bonds, line failure through the units in horizontal bending, crushing of the bed mortar joint at large crack rotations and sliding [1, 9]. 0 2 4 6 8 10 12 14 16 18 0 5 10 15 20 25 Stress S22 (MPa) Time (steps)
Numerical analysis of the out-of-plane behavior of unreinforced masonry walls 86