scieee AI-readable full text Open interactive document viewer

mRNA-activated matrices encoding transcription factors as primers of cell differentiation in tissue engineering

Martínez Ledo, Adriana; Senra, Ana; Rilo Álvarez, Héctor; Borrajo Alonso, Erea; Vidal Figueroa, Anxo; Alonso Fernández, María José; García Fuentes, Marcos

Abstract

Gene-activated matrices (GAMs) encoding pivotal transcription factors (TFs) represent a powerful tool to direct stem cell specification for tissue engineering applications. However, current TF-based GAMs activated with pDNA, are challenged by their low transfection efficiency and delayed transgene expression. Here, we report a GAM technology activated with mRNAs encoding TFs SOX9 (cartilage) and MYOD (muscle). We find that these mRNA-GAMs induce a higher and faster TF expression compared to pDNA-GAMs, especially in the case of RNase resistant mRNA sequences. This potent TF expression was translated into a high synthesis of cartilage- and muscle-specific markers, and ultimately, into successful tissue specification in vitro. Additionally, we show that the expression of tissue-specific markers can be further modulated by altering the properties of the mRNA-GAM environment. These results highlight the value of this GAM technology for priming cell lineage specification, a key centerpiece for future tissue engineering devices.

Full text

1 mRNA-Activated Matrices Encoding Transcription Factors as Primers of Cell Differentiation in Tissue Engineering Adriana M. Ledoa, Ana Senrab, Héctor Rilo-Alvareza, Erea Borrajoc, Anxo Vidalc, Maria J. Alonsoa, Marcos Garcia-Fuentesa,* a Department of Pharmacology, Pharmacy and Pharmaceutical Technology, IDIS Research Institute, CiMUS Research Institute, University of Santiago de Compostela, 15782 Santiago de Compostela, Spain b Histology Unit, CIMUS Research Institute, University of Santiago de Compostela, 15782 Santiago de Compostela, Spain c Department of Physiology, IDIS Research Institute, CIMUS Research Institute, University of Santiago de Compostela, 15782 Santiago de Compostela, Spain * Corresponding author: marcos.gar[email protected] ABSTRACT Gene-activated matrices (GAMs) encoding pivotal transcription factors (TFs) represent a powerful tool to direct stem cell specification for tissue engineering applications. However, current TF-based GAMs activated with pDNA, are challenged by their low transfection efficiency and delayed transgene expression. Here, we report a GAM technology activated with mRNAs encoding TFs SOX9 (cartilage) and MYOD (muscle). We find that these mRNA-GAMs induce a higher and faster TF expression compared to pDNA-GAMs, especially in the case of RNase resistant mRNA sequences. This potent TF expression was translated into a high synthesis of cartilage- and muscle-specific markers, and ultimately, into successful tissue specification in vitro. Additionally, we show that the expression of tissue-specific markers can be further modulated by altering the properties of the mRNA-GAM environment. These results highlight the value of this GAM technology for priming cell lineage specification, a key centerpiece for future tissue engineering devices. Key words: GAMs, 3D transfection, mRNA, transcription factors, lineage priming, tissue engineering Polymer matrices have been largely explored as tissue engineering devices. Since the Food and Drug Administration (FDA) approval of the first collagen-based dermal regeneration template Omnigraft®(1) (Integra Life Sciences, Plainsboro NJ), several material systems have reached the market and paved their way into the clinical setting. Although the first devices largely consisted of biocompatible scaffolds used as fillers or protective patches, polymer matrices soon started to comprise growth factors and other recombinant proteins that help direct the regenerative process. Examples of this successful approach include a rhBMP-7-loaded collagen carrier (OP- 1™); a rhBMP-2 loaded collagen sponge (Infuse®); and a sodium carboxymethylcellulose-based gel loaded with rhPDGF (Regranex®)(2). However, these factors are often administered at high doses, to overcome their short half-life, and current formulations offer poor control over their release profiles. This in turn leads to side effects, among which, the risk of malignancies is one of the biggest concerns(3–5). 2 Trying to overcome these limitations, researchers started to explore the use of gene therapy as an alternative strategy to recombinant protein delivery, and the concept of Gene Activated Matrix (GAM) was described(6). Initially, GAMs were based on plasmid DNA (pDNA), free or complexed to non-viral formulations, encoding the growth factor of interest. This pDNA was loaded within a polymer matrix from which it would be released, transfecting the surrounding cells and inducing the consequent sustained and localized expression of the desired factor(7). Nevertheless, while non-viral delivery of pDNA is preferred over viral vectors due to safety concerns, non-viral formulations are characterized by low gene transfer efficiencies, which hamper their clinical success. This scenario has prompted the development of RNA-based GAMs, based on the superior gene transfer capacity of RNA compared to that of DNA(8). In this regard, different RNA GAMs were explored, ranging from siRNA and miRNA-GAMs(7), to the more recent mRNA-GAMs first described by Elangovan(9). In this work, the authors used chemically modified mRNA encoding the growth factor BMP-2, to study the bone regeneration in rat calvarial defects and demonstrated its superior biocompatibility and regenerative capacity compared to traditional pDNA-GAMs. Subsequent works explored the use of other growth factors and material systems to fabricate mRNA-based GAMs, further consolidating their value(10,11). Compared to growth factors, transcription factors (TFs) have higher potency and specificity to drive cell reprogramming and directed differentiation(12–16). Realizing their potential for tissue engineering applications, researchers have investigated the use of GAMs encoding pivotal TFs in musculoskeletal development, and established TF-activated GAMs as promising alternatives to “traditional” growth factor-activated GAMs(17,18). Despite this, and the fact that mRNA- encoding TFs can efficiently modulate cell phenotype(16,19–21), to the best of our knowledge, TF-based GAMs have only been explored for pDNA. In this work, we describe a new kind of mRNA-GAMs, activated with lineage-specific TFs and loaded with human mesenchymal stem cells (hMSCs), to direct cell specification in injured or diseased tissues. To this end, fibrin hydrogels were activated with nanocomplexed mRNA encoding SOX9 (cartilage)(22,23) and MYOD (muscle)(24), to promote MSC chondrogenic and myogenic differentiation. Compared to previously explored TF pDNA-GAMs, we hypothesized that the rapid gene modulation induced by mRNA could trigger a faster onset of the differentiation cascades, improving the quality of the regenerated tissue and so providing therapeutic benefits compared to current technologies. Methods Cell culture Human adipose derived Mesenchymal Stem Cells (hMSCs) were acquired from tebu-bio (Le Perray-en-Yvelines, France) and ATCC (Manassas, VA, USA) and cultured in α-MEM (Gibco, Life Technologies, Carlsbad, CA, USA) supplemented with 10% fetal bovine serum (Gibco), 1% penicillin-streptomycin (Gibco) and 10 ng/ml bFGF (Peprotech, Rocky Hill, NJ, USA). Cells were detached from the plates using TrypLE solution (Gibco) and plated at 5000-7500 cells/cm2. Media was changed every 2-3 days and cells were split at 70-80% confluency. 3 Plasmid design and mRNA synthesis Yellow Fluorescent Protein (YFP) and SOX9 mRNAs were in vitro transcribed (IVT) from plasmid templates (Fig. S1). To construct the YFP plasmid, the YFP coding sequence (CDS) and a SV40 polyadenylation signal were sequentially digested from a pIRES YFP vector (Clontech, Mountain View, CA, USA) using the XhoI and SmaI sites, and ligated into a pBluescript KS (+) vector (Stratagene, San Diego, CA, USA). Digestion products were separated in agarose gels and purified with the Wizard SV Gel and PCR Clean-up system kit (Promega, Madison, WI, USA) before overnight ligation at room temperature with T4 DNA ligase (Promega). For SOX9 plasmid, the SOX9 CDS, a Kozak consensus sequence and the 3’ UTR of the α globin gene(16,25,26) were synthesized and cloned into a pCMVTnT expression vector (Promega, Madison, WI, USA) by Genewiz (South Plainfield, NJ, USA). Both plasmids were sequence-verified (Stab Vida, Caparica, Portugal) and DH5α E. Coli bacteria were transformed for their propagation. Plasmids were extracted from the bacterial cultures and purified with the NucleoSpin Plasmid Kit (Macherey- Nagel, Dueren, Germany) according to the manufacturer’s instructions. Corresponding mRNA sequences were synthesized with the Anti-Reverse Cap Analog (ARCA) technology, using the mMESSAGE mMACHINE T7 Ultra kit (Ambion, Foster City, CA, USA) following the manufacturer’s protocol. Briefly, plasmids were linearized using XhoI and BamHI restriction enzymes (Promega) and 2-7 enzyme units per µg of pDNA. Endonuclease digestion was confirmed by gel electrophoresis and 1.35 µg of linearized plasmids were used as templates for each 20 µl reaction. mRNAs were purified via phenol-chloroform extraction using Phase Lock 1.5 ml tubes (5 Prime, Hilden, Germany) followed by ethanol precipitation and quantification by Nanodrop (Thermo Fisher Scientific, Waltham, MA, USA). MYOD mRNA was purchased from Stemgent (Cambridge, MA, USA) and used as supplied. Preparation and characterization of 3DFectIN complexes For 3D transfection experiments, 50 µl of 3DfectIN® complexes (OZ Biosciences, Marseille, France), in the specified 3DFectIN: DNA/RNA ratios (µl:µg), were prepared in OptiMEM (Gibco) following the manufacturer’s instructions. Briefly, a solution containing 1 µg of mRNA/pDNA was added over a solution containing 1, 2, 3 or 4 µl of 3DFectIN® reagent in a 1/1 v/v ratio, mixed by pipetting up-down and incubated for 20 min at room temperature. Particle mean size and polydispersity index were analyzed by Dynamic Light Scattering (Nanosizer ZS®, Malvern, Worcestershire, UK) without further dilution. Distribution of the complexes within the hydrogels was assessed by fluorescence microscopy (Olympus IX51 operated with a U-RFL-T lamp) after the encapsulation of SYBR®Gold-labeled pDNA complexes. To this end, an aqueous solution of pDNA was labeled by mixing with a 50X DMSO solution of SYBR®Gold Nucleic Acid Gel Stain (Invitrogen) in a ratio 1:1 (µg:µl) and incubated for 5 min at room temperature before complexes were prepared. Hydrogel preparation and 3D transfection Human plasma derived fibrinogen and thrombin were purchased from Sigma-Aldrich (St. Louis, MO, USA). Both materials were reconstituted in, Ca2+ and Mg2+ free, phosphate buffered saline 4 (PBS) (Invitrogen) at 50 mg/ml and 100 U/ml, respectively, and further diluted with the same buffer before hydrogel formation. Fibrin hydrogels of 2 and 4 mg/ml were prepared using 2.5 U/ml of thrombin and cast in tissue culture plates (Thermo Fisher Scientific). Transfection and characterization assays were performed with 100 µl gels cast in 96 well plates. In differentiation assays, 200 µl gels were cast in 48 well plates. For 100 µl gels, 20 µl of the fibrinogen solution (20 or 40 mg/ml) were added to the bottom of the plate. Then, 10 µl of the cell suspension mixed with 50 µl of OptiMEM (control gels), the cell suspension mixed with 50 µl of 3DFectIN® complexes (gene-activated gels), or 60 µl of OptiMEM (blank gels) were thoroughly blended with fibrinogen by pipetting up-down. After this, 20 μl of the thrombin solution (12.5 U/ml) were quickly mixed with the previous hydrogel blend (1.5x106 cells/ml of gel) avoiding the formation of bubbles. Plates were placed in the cell incubator at 37°C for 1 h to allow gelation. Finally, 200 µl of culture medium were added on top of each gel. For 200 µl gels, the same procedure was followed but quantities were doubled. Scanning electron microscopy Blank and cell-seeded fibrin hydrogels were prepared as previously described (Hydrogel preparation and 3D transfection). Blank gels were frozen at -80°C after the gelation process, while hMSCs seeded gels were kept one week in culture before freezing. All gels were freezedried in a VirTis Genesis 25 ES freeze-drier (SP Industries, Warminster, PA, USA) under the following program: primary drying at -35°C for 24 h, secondary drying at 0°C for 24 h and 14 h at room temperature. Freeze-dried samples were carefully removed from the plates and metalized with iridium using a Sputer Coater Quorum Q150T-S (Guelph, Ontario, Canada). Samples were visualized in a Zeiss FESEM Ultra Plus with EDX operated at 5 kV. Cell toxicity and proliferation assays Toxicity derived from the encapsulation of hMSCs in gene-activated gels was evaluated by MTT assays (Sigma-Aldrich). Cell proliferation was investigated by monitoring the DNA content using the Quant-iT PicoGreen dsDNA assay kit (Invitrogen, Life Technologies, Carlsbad, CA, USA). hMSCs were encapsulated in fibrin hydrogels with or without 3DFectIN® complexes at a density of 1.5x105 and 1.5x106 cells/ml for MTT and PicoGreen assays, respectively. For MTT assays, gels were cultured during 24 and 48 h and PicoGreen assays were run for 12, 24 and 48 h (short assays) or 3, 7 and 10 days (long assays), preserving some gels for day 0 controls. At the desired time points, gels were digested with 100 µl of a 2.5% trypsin solution (30 min, 37°C) and transferred to 2 ml tubes. In the case of MTT assays, formazan crystals were solubilized with a 1/1 v/v mix of 20% sodium dodecyl sulfate (SDS) in PBS and isopropanol by vortexing for 15 min at 2000 rpm in an Eppendorf MixMate® (Eppendorf, Hamburg, Germany) followed by absorbance reading (570 nm with 690 wavelength correction) in a Multiskan GO spectrophotometer (Thermo Scientific). The reading values in gene-activated gels were converted to the percentage of the control (non-activated) gels. For proliferation assays, DNA was extracted with a sequential lysis process using an SDS solution (0.1% w/v in PBS) for the first step and a Triton X-100 solution (1% in PBS) for the second step. Samples were vortexed in an Eppendorf MixMate® (15 min at 2000 rpm for each step) to help extraction. Fluorescence readings were performed at 480/520 excitation/emission wavelengths in an EnVision multilabel 5 plate reader (Perkin Elmer, Whaltam, MA, USA). Blank gels were included to subtract the fluorescence background and calibration was performed against a λ DNA standard. Hydrogel degradation assay Cell-mediated degradation of fibrin hydrogels was determined by digesting the gels and measuring the change in protein content over time. Non-activated hydrogels, seeded with hMSCs, were prepared as previously described (Hydrogel preparation and 3D transfection) and incubated in culture media at 37°C and 5% CO2 for 5 days. At day 1, 2 and 5, the media was aspirated, and gels were digested with 100 µl of a 2.5% trypsin solution (30 min, 37°C). After digestion, samples were diluted with water and the protein content was quantified as described in Supplementary information. Percentage weight change was normalized to day 0. Chondrogenic differentiation Chondrogenesis assays were performed in hMSCs below passage 10. For experiments evaluating the kinetics of chondrogenic marker expression, 2 and 4 mg/ml hydrogels were cast in 96 well plates and cultured for 7 and 21 days in Complete Chondrogenic Medium (CCM) consisting of DMEM high-glucose 1 mM pyruvate (Gibco), 100 nM dexamethasone (Sigma-Aldrich), 50 μg/ml ascorbic acid 2-phosphate (Sigma-Aldrich), 40 μg/ml L-proline (Sigma-Aldrich), 1% ITS Premix supplement (Becton Dickinson), 1% penicillin/streptomycin (Gibco) and 10 ng/ml transforming growth factor-β3 (TGF-β3) (Peprotech). Hydrogels (100 µl) were activated with two doses of SOX9 mRNA and pDNA, namely 1 and 0.25 µg per gel, and at desired time points, total RNA was extracted to check for the presence of chondrogenic markers SOX9, aggrecan (ACAN) and collagen type II (COL2A1) by qRT-PCR. For experiments evaluating the quality of the cartilagelike tissue, fibrin hydrogels of 2 mg/ml (0.5 µg mRNA per 200 µl gel) were cast in 48 well plates and cultured in CCM, and CCM without TGF-β3 (Incomplete Chondrogenic Medium, ICM), for 21 days. At the end of the experiments, SOX9-activated gels were retrieved from the plates and the expression of chondrogenic markers was assessed and compared to non-activated gels cultured in the same conditions. Gene expression of SOX9, ACAN, COL2A1 and collagen type X (COLX) was assessed by qRT-PCR. Alcian blue staining and collagen type II immunohistochemistry (IHC) were used to analyze the deposition of extracellular matrix. Media was changed every 3 days in both experiments. Myogenic differentiation Two protocols were assayed for myogenic differentiation. For both protocols, fibrin hydrogels of 2 and 4 mg/ml were cast in 48 well plates and cultured for 14 days. In the first protocol, hydrogels were activated with 0.5 µg of MYOD mRNA per gel and cultured in complete growth media for the first day, changing to DMEM high glucose, supplemented with 2% horse serum (Gibco) and 1% penicillin-streptomycin, for the rest of the assay. In the second protocol, hydrogels were activated with 0.25 µg of MYOD and cultured in α-MEM supplemented with 5% fetal bovine serum and 1% penicillin-streptomycin for the first 7 days (growth phase) switching to DMEM high glucose, supplemented with 2% horse serum, 1% penicillin-streptomycin and 10 ng/ml insulin growth factor 1 (IGF-1) (Peprotech), for the rest of the assay (differentiation 6 phase). At the end of the experiments, hydrogels were retrieved and the expression of myogenic markers was assessed and compared to non-activated gels cultured in the same conditions. Gene expression of myogenic differentiation protein 1 (MYOD), myogenin (MYOG), cadherin 15 (CDH15), myosin heavy chain 2 (MYH2) and myosin heavy chain 3 (MYH3) was evaluated by qRT- PCR whereas myosin IHC was used to analyze myosin protein expression. Media was changed every 2 days in both experiments. Total RNA extraction Two hydrogels (100 µl) or one hydrogel (200 µl) per condition were used for RNA extraction. Hydrogels were removed from the plates with the help of a spatula and placed in 1.5 ml tubes. In transfection experiments, gels were washed with 0.5 ml of PBS and centrifuged in an Eppendorf 5430R centrifuge (1500 x g, 5 min, 4°C) to remove any remaining media before the extraction. In the case of chondrogenic differentiation experiments, gels and pellets were washed with PBS, digested with 700 collagenase units (Gibco) for 15 min at 37°C and washed again, before starting the extraction protocol. Centrifugation speed during the washing steps was set at 1500 x g and 100 x g for the gels and pellets, respectively. For each RNA extraction, 350 µl of lysis buffer were used and samples were digested by vortexing for 15 min at 2000 rpm in an Eppendorf MixMate® with the help of two 2.8 mm stainless steel grinding balls (Ops Diagnostics, Lebanon, NJ, USA). Cell lysates were extracted with the SPEEDTOOLS total RNA extraction kit (Biotools, Madrid, Spain) following the manufacturer’s instructions. RNA was quantified by UV absorbance using a Nanodrop 2000 spectrophotometer (Thermo Scientific). cDNA synthesis and qRT-PCR Reverse transcription was carried out using 100-500 ng of total RNA per sample in a 30 µl final reaction volume. First, total RNA was mixed with random primers and dNTPs (Invitrogen) and kept at 65°C for 5 min. Samples were then incubated with a mix of RNase OUT, 5x first strand buffer and DTT (Invitrogen) for 2 min at 37°C and subsequently placed on ice. Finally, reverse transcriptase (M-MLV, Invitrogen) was included and the cycle was continued as follows: 10 min at 25°C, 50 min at 37°C and 15 min at 70°C. The resulting cDNA (5-30 ng) was used to assemble qRT-PCR reactions in a final volume of 20 µl containing Universal PCR Mastermix and TaqMan assays (Applied Biosystems, Table S1). The thermal cycling was done in a StepOne Real Time PCR System (Applied Biosystems) performing a 10 min hold at 95°C followed by 40 cycles of 15 sec at 95°C and 1 min at 60°C. No template controls were used in each reaction as negative control. Gene expression values were normalized to internal controls (β-actin and GAPDH) and presented as a fold change relative to cells plated in 2D before the experiments using the comparative 2-∆∆Ct method(27). In the experiments evaluating SOX9 expression kinetics, the maximum levels of gene expression detected for each condition were arbitrary set as 100% expression. The expression obtained at the other two remaining time points was expressed as a percentage relative to that maximum expression. 7 Immunohistochemistry Hydrogels were retrieved from tissue culture plates, washed with PBS and fixed with 10% buffered formalin at room temperature for less than 24 h. After fixation, samples were maintained in 70% ethanol before dehydration and paraffin sectioning. Sections of 4 µm thickness were cut and allowed to adhere to poly-L-lysine treated glass slides overnight at 55 °C. Before staining, sections were dewaxed in xylene and hydrated with graded ethanol. Samples from chondrogenic differentiation experiments were stained for deposited sGAG and collagen content, with Alcian blue (pH 2.5) and Sirius red, respectively. Immunohistochemical staining (IHC) was performed to check for the presence of collagen type II (II-II6B3, DSHB, Iowa City, IA, USA) and myosin heavy chain (clone MY-32 Sigma-Aldrich), after chondrogenic and myogenic differentiation experiments, respectively. Antigen retrieval was performed in Tris-EDTA buffer during 20 min at 95°C in a PT Link (Agilent, Santa Clara, CA, USA). Samples were pre-treated with hydrogen peroxide and blocked with serum free protein block (Dako; Agilent, Santa Clara, CA, USA). Primary antibodies were diluted 1:100 in antibody diluent (Dako) and incubated overnight at 4°C followed by the incubation with goat secondary antibodies labeled with HRP (Dako) at 1:100 for 1 h and the staining with 3,3’-diaminobenzidine (DAB). Negative controls for histology consisted of hydrogels maintained in regular culture conditions. IHC negative controls were obtained by omitting the primary antibodies (Fig. S2). All samples were observed using an Olympus BX43 microscope equipped with an Olympus XC50 camera. ! Statistical Analysis The statistical analysis was performed using GraphPad Prism. Where applicable, data are reported as the mean ±SD. Data were compared using One- or Two-way ANOVA and p-values less than 0.05 were considered to be statistically significant. Results Synthesis and characterization of gene activated matrices (GAMs) The main concept of this work was to develop GAMs activated with mRNA coding for transcription factors (TFs) that are master regulators of cell lineage specification: SOX9 (cartilage) and MYOD (muscle). In order to generate these GAMs, mRNA sequences were nanocomplexed with 3DFectIN® and loaded within fibrin-based hydrogels together with human mesenchymal stem cells (hMSCs). The same GAMs, activated with pDNA, were used as a benchmark throughout the study (Fig. 1A). In an initial characterization step, GAMs were prepared with polynucleotides encoding the reporter sequence Yellow Fluorescent Protein (YFP), and different 3DfectIN:polynucleotide ratios were evaluated in terms of nanocomplex size, polydispersity index, and payload association efficiency. Increasing 3DfectIN:polynucleotide ratios from 1:1 to 4:1 (µl:µg) produced smaller and less polydisperse mRNA nanocomplexes, whereas pDNA nanocomplexes followed an opposite trend (Fig. 1B, S3B). Ratio 1:1 exhibited the best compromise for both polynucleotides regarding particle size and polydispersity index, but this ratio showed an incomplete complexation of the 8 polynucleotides, that was not observed for the other ratios (Fig. 1C, S3A). Consequently, only ratios 2:1 to 4:1 were further used to screen the influence of 3DFectIN:polynucleotide ratios and polynucleotide doses on GAM transfection efficiency. These transfection experiments were performed in U87MG cells and showed that mRNA induced a much higher YFP expression than pDNA, as assessed by fluorescence microscopy (Fig. S4A). In addition, cells loaded with either the highest mRNA dose (2 µg) or the highest 3DFectIN:mRNA ratio (4:1) formed clumps and lost their spindle morphology, suggesting that mRNA nanocomplexes loaded with 1 µg mRNA at a 3DFectIN:mRNA ratio of 3:1, provided the best balance between cytotoxicity and transfection efficiency (Fig. S4A, B). In order to confirm this result, SOX9 mRNA and pDNA nanocomplexes prepared at 2:1 and 3:1 ratios, were loaded within the matrices and the transgene expression was determined by quantitative real-time polymerase chain reaction (qRT-PCR). As expected, mRNA nanocomplexes prepared at 3:1 ratio showed the higher transfection efficiency (Fig. S4C) and hence this ratio was selected for further experiments with hMSCs. Although a 2:1 ratio resulted in pDNA complexes below the micrometric size and effectively encapsulated the payload (Fig. S3), a 3:1 ratio was also selected for pDNA complexes, since it was able to transfect as efficiently (Fig. S4) and provided a more consistent benchmark for mRNA-activated matrices prepared at a 3:1 ratio. GAMs prepared at two fibrin concentrations (2 and 4 mg/ml) presented a highly porous and fibrillar micro-architecture (Fig. 1D) where the nanocomplexes were homogeneously distributed (Fig. 1E, S3C). An increased hydrogel porosity, accompanied by a thicker fibrillar network, was observed in both MSC-seeded gels compared to their blank counterparts, probably due to cellmediated hydrogel remodeling and matrix deposition. Since hydrogel remodeling is linked to cell-mediated degradation, an experiment was performed to monitor the mass loss of cellseeded hydrogels over time. Although no significant differences could be observed between both types of matrices after 24 h, the percentage of mass recovery was lower for 2 mg/ml fibrin matrices after 2 and 5 days, indicating their faster degradation (Fig. 1F). Cytotoxicity assays, carried out at 24 h and 48 h, showed no significant impact of the mRNA complexation reagent on hMSC viability regardless of the fibrinogen concentration (Fig. S5A). Additionally, DNA quantification assays confirmed that the inclusion of mRNA complexes within the matrices had no significant long-term effect on cell growth compared to control matrices, and that both fibrinogen concentrations induced very similar cell proliferation rates (Fig. S5B). Finally, hMSC transfection within mRNA GAMs prepared at 3:1 ratio, was evaluated qualitatively by YFP reporter expression, confirming the results obtained for the model cell line (Fig. 1G). Effect of polynucleotide type and fibrinogen concentration on GAM gene expression Having confirmed that mRNA-GAMs were able to induce YFP expression in hMSCs, with negligible effects on their viability, we next characterized the influence of the fibrin concentration and the type of polynucleotide (mRNA vs. pDNA) on transfection efficiency. We first sought to determine whether the transfection results observed for SOX9 in the U87MG model cell line (Fig. S4), could be reproduced in hMSCs. For this, SOX9 expression in hMSCs entrapped within SOX9-GAMs was quantified by qRT-PCR. In line with the previous results, mRNA-GAMs induced around a two-fold increase in SOX9 expression in hMSCs compared to 9 pDNA-GAMs. Conversely, no differences in transgene expression levels could be observed between matrices with 2 mg/ml and 4 mg/ml of fibrinogen, independently of whether they were activated with mRNA or pDNA (Fig. 2A). Importantly, both GAMs induced a remarkable upregulation (>5·104-fold increases) of SOX9 as compared to control cells, seeded within nonactivated matrices. In order to test the effect of RNase resistant mRNA sequences on transfection efficiency, we next performed a set of transfection experiments with MYOD- matrices, activated with methylated MYOD mRNA. As expected, MYOD relative expression, as assessed by qRT-PCR, was very potent in these matrices, achieving levels that were eight orders of magnitude above the controls (Fig. 2B). For both SOX9 and MYOD mRNA-GAMs, we verified that the amount of mRNA extracted from the nanocomplexes during sample processing was not enough to contaminate the total RNA extracted from the cells and thus it was not interfering with the qRT-PCR results (Supplementary methods, Fig. S6). Gene expression kinetics was mostly determined by the type of polynucleotide, regardless of the matrix concentration. Indeed, despite the variability derived from the use of different stem cell and mRNA batches across the experiments, both SOX9 GAMs showed consistently opposite transgene expression trends: transgene expression levels peaked at early time points for mRNA- activated matrices and at late time points for pDNA-activated matrices (Fig. 2C). Interestingly, contrary to the gradual decay in transcription factor expression observed in SOX9-mRNA matrices over time (12-48 h), the MYOD expression induced by MYOD-mRNA matrices was maintained over the entire experiment (48 h) (Fig. 2D). Although both SOX9 and MYOD have positive auto-regulation mechanisms(28,29), different rates of these positive feedback loops may result in the different transgene expression levels obtained for both genes. Additionally, the fact that MYOD mRNA was chemically modified to increase its resistance to RNases, compared to the non-modified SOX9 mRNA sequences, may also contribute to the different kinetics of transgene expression. Chondrogenic differentiation We next sought to explore whether we could use the differences in gel remodeling and transgene expression kinetics to maximize the expression of tissue differentiation markers. To this end, mRNA- and pDNA-GAMs encoding SOX9 were assayed for chondrogenic differentiation. We first conducted a screening experiment to understand the kinetics of chondrogenic marker expression induced by our devices, and to select the best conditions for further analysis. We tested the two concentrations of fibrin hydrogels (2 and 4 mg/ml) with both types of polynucleotides (pDNA and mRNA) at two different doses (1 and 0.25 µg per 100 µl hydrogel). As a reference standard culture for chondrogenic differentiation, we included highdensity cell pellet cultures. Gels and pellets were cultured in Complete Chondrogenic Medium (CCM) for 7 and 21 days and the expression of chondrogenic markers SOX9, aggrecan (ACAN) and collagen type-II (COL2A1), was assessed by qRT-PCR (Fig. 3). At day 7, gels activated with 1 µg of pDNA produced the highest SOX9 upregulation followed by gels activated with 1 µg of mRNA. Gels activated with 0.25 µg of both pDNA and mRNA induced a lower SOX9 expression, although their levels were still higher than those of standard cell pellet cultures. The highest ACAN expression at this time point was obtained for both mRNA activated hydrogels, with no 16 producing cells in vitro. Clin Exp Med2014;15(4):501–9. 21. Aini H, Itaka K, Fujisawa A, Uchida H, Uchida S, Fukushima S, et al. Messenger RNA delivery of a cartilage-anabolic transcription factor as a disease-modifying strategy for osteoarthritis treatment. Sci Rep 2016;6(November 2015):18743. 22. Dy P, Wang W, Bhattaram P, Wang Q, Wang L, Ballock RT, et al. Sox9 directs hypertrophic maturation and blocks osteoblast differentiation of growth plate chondrocytes. Dev Cell 2012;22(3):597–609. 23. Bi W, Deng JM, Zhang Z, Behringer RR, Crombrugghe B De. Sox9 is required for cartilage formation. Nat Genet 1999;22(may):85–9. 24. Davis RL, Weintraub H, Lassar AB. Expression of a single transfected cDNA converts fibroblasts to myoblasts. Cell 1987;51(6):987–1000. 25. Kozak M. An analysis of 5’-noncoding sequences from 699 vertebrate messenger rNAS. Nucleic Acids Res 1987;15(20):8125–48. 26. Holcik M, Liebhaber S a. Four highly stable eukaryotic mRNAs assemble 3’ untranslated region RNA-protein complexes sharing cis and trans components. Proc Natl Acad Sci U S A 1997;94(6):2410–4. 27. Pfaffl MW. A new mathematical model for relative quantification in real-time RT-PCR. Nucleic Acids Res 2001;29(9):45e – 45. 28. Tapscott SJ. The circuitry of a master switch : Myod and the regulation of skeletal muscle gene transcription. Development 2005;132:2685–95. 29. Mead TJ, Wang Q, Bhattaram P, Dy P, Afelik S. A far-upstream ( -70 kb ) enhancer mediates Sox9 auto-regulation in somatic tissues during development and adult regeneration. Nucleic Acids Res 2013;41(8):4459–69. 30. Schiaffino S, Rossi AC, Smerdu V, Leinwand LA, Reggiani C. Developmental myosins: expression patterns and functional significance. Skelet Muscle 2015;1–14. 31. Elangovan S, Khorsand B, Do AV, Hong L, Dewerth A, Kormann M, et al. Chemically modified RNA activated matrices enhance bone regeneration. J Control Release 2015;218:22–8. 32. Andries O, De Filette M, Rejman J, De Smedt SC, Demeester J, Van Poucke M, et al. Comparison of the gene transfer efficiency of mRNA/GL67 and pDNA/GL67 complexes in respiratory cells. Mol Pharm 2012;9(8):2136–45. 33. Kypriotou M, Fossard-Demoor M, Chadjichristos C, Ghayor C, de Crombrugghe B, Pujol J- P, et al. SOX9 exerts a bifunctional effect on type II collagen gene (COL2A1) expression in chondrocytes depending on the differentiation state. DNA Cell Biol 2003;22(2):119–29. 34. Harada A, Mallappa C, Okada S, Butler JT, Baker SP, Lawrence JB, et al. Spatial reorganization of myogenic regulatory sequences temporally controls gene expression. Nucleic Acids Res 2015;43(4):2008–21. 35. Cho HC, Mallappa C, Hernández-Hernández JM, Rivera-Pérez JA, Imbalzano AN. Contrasting roles for MyoD in organizing structures during embryonic skeletal muscle development. Dev Dyn 2015;244(1):43–55. 36. Takahashi K, Yamanaka S. Induction of pluripotent stem cells from mouse embryonic and adult fibroblast cultures by defined factors. Cell 2006;126(4):663–76. 37. Huebsch N, Arany PR, Mao AS, Shvartsman D, Ali OA, Bencherif SA, et al. Harnessing traction-mediated manipulation of the cell/matrix interface to control stem-cell fate. Nat Mater 2010;9(6):518–26. 38. Chaudhuri O, Gu L, Klumpers D, Darnell M, Bencherif SA, Weaver JC, et al. Hydrogels with tunable stress relaxation regulate stem cell fate and activity. Nat Mater 2015;15(3):326– 34. 39. Mao AS, Shin JW, Mooney DJ. Effects of substrate stiffness and cell-cell contact on mesenchymal stem cell differentiation. Biomaterials 2016;98:184–91. 40. Almalki SG, Agrawal DK. Effects of matrix metalloproteinases on the fate of mesenchymal stem cells. Stem Cell Res Ther 2016;1–12. 17 41. Ahmann KA, Weinbaum JS, Ph D, Johnson SL, Tranquillo RT, Ph D. Fibrin degradation enhances vascular smooth muscle cell proliferation and matrix deposition in fibrin-based tissue constructs fabricated in vitro. Tissue Eng Part A 2010;16(10). 42. Page-McCaw A, Ewald AJ, Werb Z. Matrix metalloproteinases and the regulation of tissue remodelling. Nat Rev Mol Cell Biol 2007;8(3):221–33. 43. Oh J, Takahashi R, Adachi E, Kondo S, Kuratomi S, Alexander DB, et al. Mutations in two matrix metalloproteinase genes , MMP-2 and MT1-MMP , are synthetic lethal in mice. Oncogene 2004;23:5041–8. 44. Ghone N V., Grayson WL. Recapitulation of mesenchymal condensation enhances in vitro chondrogenesis of human mesenchymal stem cells. J Cell Physiol 2012;227(11):3701–8. 45. Ray P, Chapman SC. Cytoskeletal reorganization drives mesenchymal condensation and regulates downstream molecular signaling. PLoS One 2015;10(8):1–24. 46. Bian L, Guvendiren M, Mauck RL, Burdick JA. Hydrogels that mimic developmentally relevant matrix and N-cadherin interactions enhance MSC chondrogenesis. Proc Natl Acad Sci 2013;110(25):10117–22. 47. Cosgrove BD, Mui KL, Driscoll TP, Caliari SR, Mehta KD, Assoian RK, et al. N-cadherin adhesive interactions modulate matrix mechanosensing and fate commitment of mesenchymal stem cells. Nat Mater 2016;15(12):1297–306. 48. Engler AJ, Sen S, Sweeney HL, Discher DE. Matrix elasticity directs stem cell lineage specification. Cell 2006;126(4):677–89. 49. Engler AJ, Griffin MA, Sen S, Bönnemann CG, Sweeney HL, Discher DE. Myotubes differentiate optimally on substrates with tissue-like stiffness: Pathological implications for soft or stiff microenvironments. J Cell Biol 2004;166(6):877–87. 50. Page RL, Malcuit C, Vilner L, Vojtic I, Shaw S, Hedblom E, et al. Restoration of skeletal muscle defects with adult human cells delivered on fibrin microthreads. Tissue Eng Part A 2011;17(21–22):2629–40. 51. Heher P, Maleiner B, Prüller J, Teuschl AH, Kollmitzer J, Monforte X, et al. A novel bioreactor for the generation of highly aligned 3D skeletal muscle-like constructs through orientation of fibrin via application of static strain. Acta Biomater 2015;24:251–65. 52. Chen S, Nakamoto T, Kawazoe N, Chen G. Engineering multi-layered skeletal muscle tissue by using 3D microgrooved collagen scaffolds. Biomaterials 2015;73:23–31. 18 Figure 1 19 Figure 2 20 Figure 3 21 Figure 4 22 Figure 5 23 Figure captions Figure 1. mRNA-GAMs promote stem cell-mediated remodeling and transfection. A) Scheme of the therapeutic concept proposed: human mesenchymal stem cells (MSCs) and mRNA-loaded nanocomplexes (NCs) encoding key transcription factors (TFs) are encapsulated within in situ gelling fibrin matrices. Transfection occurs when MSCs invade the matrix leading to an enforced TF expression and cell phenotype specification. Objects are not drawn to scale. B) Representative size intensity distribution of mRNA and pDNA 3DFectIN® NCs prepared at 3:1 3DFectIN:polynucleotide ratio (µl:µg) as measured by DLS. C) Gel displacement assay showing the effective association of Yellow Fluorescent Protein (YFP) pDNA to NCs prepared at 3:1 ratio. No pDNA band is detected after loading the NCs in the agarose gel (left lane) unless NCs are previously incubated with heparin to promote pDNA displacement (right lane). D) SEM analysis of the microarchitecture of fibrin matrices immediately after preparation (blank fresh) and after one week in culture with (+MSCs) and without cells (blank cultured). Scale bar = 20 µm for all the images. E) Fluorescence micrographs of SYBR®Gold labelled pDNA NCs (3:1 ratio) loaded into GAMs prepared at two different fibrin concentrations (2 and 4 mg/ml). Scale bar = 50 µm for all the images. F) Degradation rates of 2 and 4 mg/ml fibrin matrices loaded with hMSCs (Two-way ANOVA, n = 3, **P<0.01). Data are shown as mean and standard deviation of three independent experiments at 3:1 3DFectIN:mRNA ratio. G) Representative fluorescence micrographs showing Yellow Fluorescent Protein (YFP) expression in hMSCs 24 h after encapsulation within YPF- activated mRNA-GAMs prepared at 3:1 ratio. Figure 2. GAM-induced transgene expression is determined by the type of polynucleotide regardless of matrix concentration. A) SOX9 expression 24 h after hMSCs encapsulation within SOX9-activated 2 and 4 mg/ml matrices (Two-way ANOVA, n = 6, *P<0.05, **P<0.01). B) MYOD expression 24 h after hMSCs encapsulation within MYOD-activated 2 and 4 mg/ml matrices (n=4). C) SOX9 expression kinetics of hMSCs encapsulated in 2 mg/ml and 4 mg/ml matrices activated with mRNA and pDNA (n=6). D) MYOD expression kinetics of hMSCs encapsulated in 2 mg/ml and 4 mg/ml matrices activated with RNase resistant mRNA (n=4). Gene expression levels were measured by qRT-PCR, normalized to internal controls (β-actin and GAPDH) and presented as a fold change relative to cells plated in 2D before encapsulation. Maximum levels of transgene expression over the time course shown in C were arbitrary set as 100% for each condition (i. e. time point with maximum expression), and the levels obtained at the other time points were expressed as a percentage relative to this 100%. All experiments were performed at 3:1 3DFectIN:polynucleotide ratio. Figure 3. SOX9 mRNA-GAMs induce a faster chondrogenic marker expression than pDNA- GAMs. Chondrogenic marker expression of hMSCs encapsulated within 2 and 4 mg/ml mRNA- and pDNA-activated matrices cultured for 7 days (left) and 21 days (right) in complete chondrogenic media. Two doses of mRNA were tested, namely 0.25 and 1 µg per 100 µl gel. Gene expression levels of SOX9 (A), aggrecan (B) and collagen type-II (C) were measured by qRT- PCR, normalized to GAPDH expression and presented as a fold change relative to cells plated in 2D before encapsulation. Not detected cycle thresholds are highlighted as n. d. Data are shown as mean and standard deviation of two replicates in one experiment performed at 3:1 3DFectIN:polynucleotide ratio. A two-way ANOVA was performed to compare gene expression 24 levels in mRNA and pDNA activated matrices of the same dose and concentration (*P<0.05, **P<0.01, ***P<0.001) and to compare 2 mg/ml and 4 mg/ml matrices with the same dose and genetic material (##P<0.01, ###P<0.001) (n=3). High-density cell pellet cultures are shown as a benchmark for comparison purposes. Figure 4. SOX9 mRNA- and pDNA-GAMs respond differently to TGF-β3 supplementation. Hydrogels (3:1 3DFectIN:gene ratio) were cultured for 21 days in complete and incomplete chondrogenic media (CCM and ICM, with and without TGF-β3). A) Gene expression levels of collagen type-II (COL2A1) and collagen type-X (COLX) normalized to GAPDH and presented as a fold change relative to cells plated in 2D before encapsulation. Not detected cycle threshold levels are highlighted as n. d. Data are represented as mean and standard deviation bars (n=3) and analyzed by two-way ANOVA (*P≤0.05, ****P≤0.0001). Control designates the control matrices that have the same composition as GAMs but are not loaded with gene nanocomplexes. B) Immunohistological examination of glycosaminoglycan and collagen deposition. Hydrogels were stained with alcian blue for sGAG detection. Collagen type-II was detected by immunohistochemistry. A standard cell pellet culture is shown for comparison. Images are representative of two independent experiments with three replicates per experiment. Scale bar = 20 µm for all the images. Figure 5. MYOD expression and fibrin matrix concentration jointly promote MSC myogenic maturation in MYOD-GAMs. A) Kinetics of myogenic marker expression myogenin (MYOG) and cadherin 15 (CDH15) in hMSCs cultured in MYOD-matrices (3:1 3DFectIN:mRNA ratio) for 2 days. Cells were maintained in growth media (α-MEM 10% FBS). B-C) Myogenic differentiation experiment. Hydrogels were cultured for 7 days in α-MEM (5% FBS) followed by a 7 days culture in DMEM high glucose (2% HS, 10 ng/ml IGF-1). B) Gene expression levels of myogenic markers MYOD, myogenin (MYOG), myosin heavy chain type 2 (MYH2) and myosin heavy chain type 3 (MYH3) normalized to GAPDH and presented as a fold change relative to cells plated in 2D before encapsulation. Control designates the control matrices that have the same composition as GAMs but are not loaded with gene nanocomplexes. All data are shown as means with standard deviation bars (n=3-6). Two-way ANOVA was performed to compare gene expression levels in control matrices and GAMs (*P<0.05, **P<0.01, ***P<0.001) and in 2 mg/ml and 4 mg/ml matrices (###P<0.001). C) Examination of myosin heavy chain expression by immunohistochemistry. Scale bar = 50 µm for all the images. 25 SUPPORTING INFORMATION Supplementary methods 2D Lipofectamine® 2000 transfection For 2D transfections, cells were plated in 96 well plates approximately 12 h prior to transfection at a density of 90000 (U87MG) or 75000 (hMSCs) cells/cm2. Four hours before transfection, the media was changed to OptiMEM reduced serum medium (Gibco). Then, 50 µl of Lipofectamine complexes (Gibco), at 0.5:1 Lipofectamine:DNA/RNA ratios (µl:µg), were prepared in OptiMEM following the manufacturer’s instructions. Briefly, a solution containing 1 µg of mRNA/pDNA was added over a solution containing 0.5 µl of Lipofectamine® 2000 reagent in a 1/1 v/v ratio, mixed by pipetting up-down and incubated for 20 min at room temperature. Complexes were added over the cells, drop-by-drop, and incubated for 6 hours. Subsequently, complexes were aspirated and cells were maintained in regular growing media until analysis. The transfection reaction was escalated for plates of higher surface areas. Protein extraction from 2D cultures Cells were retrieved from the plates, pelleted by centrifugation (5 min, 15°C, 1000 rpm) and washed two times with PBS. RIPA buffer, supplemented with protease inhibitor cocktail (Sigma- Aldrich), was added to the clean pellet (0.5 ml per 60 mm dish) followed by a 20 min incubation on ice. Samples were then sonicated in a Branson Digital Sonifier 250 (30% amplitude, 5 pulses of 1 sec), centrifuged (15 min, 16000xg, 4°C) and supernatants were collected for further analysis. Protein concentration was determined by UV absorbance using a Multiskan GO spectrophotometer (Thermo Scientific) and following the Bradford method. A bovine serum albumin (BSA) calibration curve and the 590/450 nm linearization method[1] were used for quantification. Western blot Protein extracts (25-50 µg) were mixed with 5x Laemmli buffer, denatured at 95°C in a Thermoblock for 5 min and separated in 10% PAGE gels. Then, proteins were electroblotted onto a PVDF membrane using a semi-dry blotter (Sigma-Aldrich) operated at 1.2 mA/cm2 membrane for 1 h. Non-specific binding sites were blocked for 2 hours at room temperature with 5% nonfat milk in 0.05% TNT buffer. The membrane was incubated overnight at 4°C with SOX9 rabbit primary antibody (Santa Cruz Biotechnologies, Dallas, TX, USA) and Tubulin mouse primary antibody (Sigma-Aldrich) using a 1:500 and 1:3000 dilution in 1% TNT, respectively. The membrane was then washed three times with 1% TNT for 10 min and further incubated for 45 min with HRP-conjugated secondary antibodies (GE Healthcare, Chicago, IL, USA), at room temperature and 1:20000 dilution in 0.5% TNT. After three more washes with 0.5% TNT, the immunoblots were finally visualized following the addition of HRP SuperSignal® West Dura Extended Duration Substrate (Thermo Scientific). 32 References [1] Zor, T., Selinger, Z. Anal. Biochem. 236, 302 (1996). [2] Gruber A.R. et al. Nucleic Acids Res. 36(Web Server Issue):W70-74 (2008).