scieee AI-readable full text Open interactive document viewer

In situ synthesis of fluorescent silicon nanodots for determination of total carbohydrates in a paper microfluidic device combined with laser prepared graphene heater

Ortiz Gómez, Inmaculada,Toral López, Víctor,Romero Maldonado, Francisco Javier,Orbe Payá, Ignacio De,García Ríos, Antonio,Rodríguez Santiago, Noel,Capitán Vallvey, Luis Fermín,Morales Santos, Diego Pedro,Salinas Castillo, Alfonso

Abstract

This work was founded by Spanish “Ministerio de Economía y Competitividad” (Projects PID2019-103938RB-I00 and CTQ2017-86125-P) and Junta de Andalucía (Projects B-FQM-243-UGR18 and P18-RT-2961). The projects were partially supported by European Regional Development Funds (ERDF).

Full text

In situ synthesis of fluorescent silicon nanodots for determination of total carbohydrates in a paper microfluidic device combined with laser prepared graphene heater Inmaculada Ortiz-Gómez a, c, Víctor Toral-López b, d, Francisco J Maldonado Romero b, d, Ignacio de Orbe-Payá a, c, Antonio García b, Noel Rodríguez b, d, Luís Fermín Capitán- Vallvey a, c, Diego P Morales b, c,*, Alfonso Salinas-Castillo a, c, * aECsens, Department of Analytical Chemistry, Faculty of Sciences, 18071 University of Granada, Granada, Spain. bResearch Group, Department of Electronics and Computer Technology, Faculty of Sciences, 18071 University of Granada, Spain cUnit of Excellence in Chemistry applied to Biomedicine and the Environment, University of Granada, Spain dPervasive Electronics Advanced Research Laboratory, University of Granada, 18071 Granada, Spain *Corresponding author: E-mail address: a[email protected] (Alfonso Salinas Castillo) and [email protected] (Diego P. Morales) Abstract We report a simple, rapid, low-resource and one-step method for formation of fluorescent silicon nanodots (SNDs) in a microfluidic paper-based analytical device (µPAD) incorporated in a reusable, portable and flexible heater for determination of total carbohydrates. The synthesis of SNDs is based on the redox reaction between (3- aminopropyl) triethoxysilane (APTS) reagent and carbohydrates, which act as a reducer. The graphene-based heater was fabricated by laser ablation of Kapton polyimide. Thereby, the developed system heat the µPAD during the synthesis of SNDs at 80ºC for 30 min. The blue emitting SNDs formed have an emission peak wavelength at 475 nm. We used a digital camera and smartphone for the quantitative analysis of total carbohydrates expressed such as index of glucose or fructose with grey scale value as the analytical parameter. Under the optimal conditions, the method has a low detection limit (0.80 µM for glucose and 0.51 µM for fructose, respectively), and a linear response (10-200 µM for glucose and 10-100 µM for fructose). The method has been applied to the determination of glucose in biological fluids (serum and urine samples). In addition, determination of total carbohydrates in commercial juices and teas has been carried out. Keywords: Silicon nanodots; Total carbohydrates; Color measurement; µPAD; Smartphone; Laser Induced Graphene heater; Laser-scribing 1. Introduction Microfluidic paper-based analytical devices (µPADs) [1] have recently received a huge attention for the design of chemical analysis platforms due to their inherent advantages such as eco-friendly support, manipulation of small volumes of fluids reducing the consumption of samples and reagents, minimization of the complexity of analytical procedures, reduction of the assay time, portability, wearability, lower cost per test, higher sensibility and integration into miniaturized analytical devices, among others [2] [3]. Thereby, microfluidic technologies have been employed in developing point of care (POC) diagnostics [4], [5], [6]. The integration of various emerging functional nanomaterials in µPADs has opened the possibility of expanding their potential. For example, advanced diagnostic technologies, such as POC diagnostics use nanomaterials for optical or electrochemical detection of multiple analytes or markers [7]. Moreover, multiple conventional detection techniques, such as colorimetric detection fluorescence, electrochemical detection, surface-enhanced Raman Spectroscopy have been integrated into µPAD for POCT assays [8],[9], [10],[11], [12]. In this way, semiconductor materials such as silicon, have emerged as a new nanomaterial to construct luminescent probes on the basis of their intrinsic properties: size, shape, composition, surface modification, high luminescence, strong photostability, good biocompatibility and low toxicity [13], [14]. Current research efforts focus on the development of silicon materials for a diverse range of applications, such as batteries, photocatalysis, plasmon enhanced spectroscopy, optical devices, biological imaging screening and sensors, among others [15]–[18]. In this sense, silicon nanodots (SNDs) have a great potential as novel nanomaterials to fabricate fluorescent probes for sensing. However, studies on SNDs are limited due to their complicated synthesis procedures, strict experimental conditions and use of costly equipment involved in the fabrication [13], [19]–[21]. Different versatile methods have been developed to produce silicon nanodots, for example solution-phase reductive strategy, sonochemical synthesis, microware irradiation, mechanochemical method, laser ablation, microemulsion, and plasma-assisted aerosol precipitation [22]–[27]. Theses methodologies require complicated procedures, harsh experiment conditions and costly equipment. For example, microwave method requires high temperature (~ 160ºC), high pressure (~10-15 times atmospheric pressure) and costly microware equipment to produce silicon nanoparticles [28]. Thus, simple and eco-friendly synthesis strategies which eliminate or reduce the use of chemical compounds as well as energy exhaustive processes are highly desirable [29]. For all this, the possibility to implement chemical reagent for nanomaterials in microfluidic platforms such as µPAD could minimize these drawbacks, allowing the in situ generation of the SNDs which reduces their aging and so, assures the reliability of the measuring process. In this direction, flexible electronics are a great allied. New materials as graphene nanoaggregates and nanowires combined with inkjet printing and laser scribing techniques, among others, ease and increase the development of miniaturized flexible devices [30], [31], [32]. One of these devices are flexible film heaters which can be used to accelerate the reaction to generate SNDs [33]. Thus, this work investigates the possibility of combing handheld readers such as smartphone with these devices to control a chemical reaction or process in a microfluidic system that increases their capabilities. Specifically, we present an application of a heater in combination with a smartphone to control a chemical reaction. A flexible Laser Induced Graphene (LIG) heater studied in a previous work [34] is combined with electronic hardware to create a system with communications capabilities that can control the temperature of the reaction. The result of this combination is a costeffective, reusable system to control the chemical reaction to determine total carbohydrates. In summary, this work describes a µPAD for direct determination of total carbohydrates with one-step synthesis of fluorescent SNDs using a reusable, cost-effective, flexible and portable LIG heater. The novelty of the proposed assay is based on the combination of paper-based microfluidic device and a LIG heater, which provides the energy necessary to heat the paper and facilitate the synthesis of SNDs. Thereby, this nonenzymatic method for the determination of total carbohydrates is based on the possibility to relate the increase of fluorescence intensity of SNDs with the concentration of carbohydrates in a sample. Therefore, the measurement of glucose and fructose, as a model compounds, can be used for the quantification of the carbohydrates in different samples by taking a photography of the µPAD using a digital camera or a smartphone under UV LED lighting. In view of the operation simplicity from the synthesis of SNDs in this assay, with this method it is possible to monitor human glucose levels in biological samples such as serum and urine. Additionally, the proposed assay results suitable to estimate total sugar content in soft drinks. Thus, the results show that the proposed device is affordable, sensitive, quick and robust, portable, simple to use and green-friendly for the use of fluorescence tools in the point of care testing. 2. Experimental 2.2. Reagents and materials Glucose, galactose, mannose, sucrose, fructose, maltose, trehalose, serine, histidine, lysine, arginine, asparagine, uric acid, urea, sodium hydroxide, sodium chloride, potassium chloride, calcium chloride, magnesium chloride, disodium hydrogen phosphate, sodium sulfate, (3-aminopropyl) triethoxysilane (APTS), Tris-HCl were from Sigma Aldrich (Madrid, Spain). All reagents used were of analytical-reagent-grade unless stated otherwise. Kapton® HN polymide films with a thickness of 125 µm was purchased from DuPontTM (Constantine, MI, USA). Conductive silver/silver chloride (Ag/AgCl) ink from Loctite (Henkel, Germany). Whatman grade 1 chromatography paper from Sigma-Aldrich was used to manufacture the µPAD. All aqueous solutions were made using purified water (18.2 MΩ·cm resistance) was obtained from a Milli-RO 12 plus Milli-Q station (Millipore, Bedford, MA, USA). 2.2.Instruments and software The fluorescence intensity of SNDs was measured with a Huawei Mate 10 lite smartphone (Huawei Technologies Co. Ltd., Shenzhen, China) after illumination with an UV LED. Custom made Android app was used to turn fluorescence intensity into colour and to analyse the region of interest (ROI) of the image. The analytical devices were fabricated on paper using a craft-cutting technique as a cost-efficient, simple and reproducible process using a 12 W CO2 laser engraver (Rayjet, Barcelona, Spain). The temperature response of the heater was also measured by applying voltage steps with Precision Source/Measurement Unit B2902 (Keysight Technologies, USA) while measuring temperature with IR camera Fluke TiS75 (Fluke Corporation, USA). Fluorescence spectrum was collected using a Varian Cary Eclipse luminescence spectrometer (Varian Ibérica, Madrid, Spain). Absorbance spectrum was obtained using a Hewlett Packard diode array spectrophotometer (model 8453; Norwalk, CT, USA). Fourier-transform infrared (FT-IR) spectra were obtained using a Bruker Tensor 27 spectrometer under Attenuated Total Reflection (ATR) configuration with spectral resolution of 2 cm-1 by accumulating 25 scans in the 4000–500 cm-1 range. To investigate the size of SNDs, dynamic light scattering (DLS) assay was performed and Zeta potential measurements of SNDs in solutions at different pH values were measured by a Malvern zetasizer. The chemical composition of SNDs synthetized on paper (Si, C, O and N) was analyzed by X-ray photoelectron spectroscopy (XPS). The XPS spectra measurements were performed by Kratos Axis ultra-DLD. Also, by energy dispersive X-ray spectroscopy (EDX) measurements, the chemical composition of SNDs was contrasted. In addition, the distribution and compositional zonation of chemical elements in the paper was elucidated by an element mapping performed by energydispersive X-ray spectroscopy (EDS). SEM images were recorded with a QuenScan 650F FEI© electronic microscope together with an Everhart-Thornley detector 8ETD. Raman spectra were acquired with a JASCO 108 NRS-5100 dispersive micro-Raman spectrometer (from JASCO, Inc., Tokio, Japan). All these studies were done at the Centre for Scientific Instrumentation (University of Granada). 2.3.Electronic device design A device for temperature control has been developed. This device must be able to measure and change the temperature of the heater and communicate with a smartphone that acts as user interface. PSoC4 (Cypress Semiconductors, USA), has been selected for this purpose as it has Bluetooth 4.0 capabilities and analog and digital reconfigurable capabilities. Thanks to this interface, the user can use the smartphone to enable or disable the heat in the device and select the temperature of the heater when it is active. Also, the actual temperature of the heater is communicated to the user through this interface. To supply power to the heater a current controlled DC/DC converter is employed. This device is controlled by a PWM generated by the PSoC4 which calculates the duty depending on the temperature measurement which is obtained from an IR thermopile sensor. The power can be supplied from two sources, a micro-USB connector or a Liion battery of 680 mAh which can supply the system for 13.6 hours. The micro-USB connector permits the use of any USB device or even an external battery for extended working time. The electronics are integrated in a rigid-flex PCB of 22.50x32.49 mm as the one shown in the Figure 1A. The rigid-flex PCB allows the integration of the temperature sensor in the housing to measure the heater temperature just over it. The heater is connected through two pads in the bottom layer. To ensure a good contact, the housing press over these pads fixing the heater at the same time. Temperature sensor is the thermopile sensor TSD305-1C55, which allows noncontact temperature sensing and I2C connection with the microcontroller. This sensor is connected through a flexible strip to place it over the heater as shown in Figure 1B. Figure 1C shows the aspect of the housing created in 3D to encapsulate the system, a window is open in this case to illuminate µPAD and measure fluorescence intensity. To be able to measure fluorescence, the case has been designed to use a smartphone at a correct focus distance. Finally, the PSoC4 can control a UV LED to excite the µPAD. The LED employed is the EOLD-365-525 (OSA Opto Light, Berlin, Germany) which emits at λ=365nm. Thanks to this feature and the design of the case, is possible to measure the sample with the device developed using a smartphone (Figure 1D). 2.4. Fabrication of the LIG heater Heaters were fabricated using Kapton® HN (DuPontTM) polyimide films with a thickness of 125 µm as raw material. A CO2 laser was used to ablate this polyimide and to obtain conductive patterns. The laser employed was a 12W CO2 laser engraver with a fixed wavelength of 10.6 µm (Rayjet, Barcelona, Spain). The laser was regulated at 20% of its maximum power and a 10% of its maximum speed, which means a power of 2.4 W and a speed of 0.15 m·s-1. The substrate was placed at 5.08 cm from the laser head, allowing spatial resolution of 25 µm. With these parameters, it is possible to obtain LIG films with a sheet resistance of 90 Ω·sq-1, while avoiding permanent deformations on the substrate. The sheet resistances were measured with B2901A Keysight source measurement unit (SMU) in a four-point measure configuration [35]. 2.5. µPAD preparation The µPADs were produced in a paper sheet using standard laboratory filter paper (Whatman no 1) by craft cutting technique [36]. The device as shown in Figure 1D, containing three separates areas, one for the sample, the second for transporting the sample and third for the synthesis of SNDs and determination of total carbohydrates. 2.6.Measurement procedure The determination of total carbohydrates expressed such as index of glucose or fructose were performed under the optimized conditions. The device was prepared by drop casting of 1 µL 98% of APTS solution onto the detection area. After, 7.5 µL of different concentrations of glucose or fructose (ranging from 10 to 1000 µM) were dropped onto the sampling area. The carbohydrate solution goes through to the detection area by capillarity. Then, the detection area of the µPAD was heat at 80ºC for 30 min to ensure complete reaction between APTS and carbohydrates to synthetize the SNDs (Figure 2). For the analysis of SNDs fluorescence intensity, the µPADs were placed under a UV LED at 365 nm wavelength using a homemade accessory designed and made by us, Figure 1C. This accessory avoids that the light from the LED interferes in the measurement of SNDs fluorescence intensity and incorporates the electronic setup. Thereby, the accessory has a hole of 4 mm diameter to let the measure of SNDs fluorescence on the detection area of the µPAD with a smartphone. The smartphone camera was placed in front of the accessory with the µPAD to take photography of the detection area where the SNDs have been synthetized after reacting with standards or real samples containing glucose and/or fructose. The setting conditions used to photograph the detection area were: ISO 500, shutter speed 1/13s, aperture value f/2.20 and focal length of 35 mm. The images acquired were processed using the same application that controls the instrument temperature. The images first were converted to gray scale and then they are analysed. First, the ROI that contains the analytical information in the detection area of 4mm is determined analysing the fluorescence intensity. Then, the software transformed each ROI into the gray scale space as the average of R, G and B coordinates from RGB (Red, Green, Blue) color space and this value was denoted by gray scale. Thus, an average of the gray scale coordinate from the pixels considered was calculated and used for the carbohydrates determination. 2.7. Treatment of real samples To evaluate the feasibility of the developed µPAD, the proposed method was applied to the determination of glucose in urine and serum, and the total carbohydrates content (glucose and fructose) in juices and teas samples. The urine samples were obtained from healthy volunteers. For glucose analysis in serum samples, artificial human serum was prepared according to the following composition: 137.5 mM NaCl, 4.2 mM NaHCO3, 3 mM KCl, 0.5 mM Na2HPO4, 0.5 mM MgCl2, 2.64 mM CaCl2 and 0.5 mM Na2SO4. The pH value of the artificial serum samples were adjusted at 7.4 [37]. For the determination of glucose in serum and urine samples, these samples were spiked with a fixed glucose standard solution. After that, the samples were filtered through 0.22 µm filter and were diluted 1:10 ratio in purified water. Also, four different soft-drinks were purchased in local markets: pineapple juice, orange juice, tomato juice, black tea and green tea were also used to validate the sensor response. The samples were shaken before opening, diluted 1:1000 with purified water and filtered by a 0.22 µm pore diameter filter. 3. Results and discussion 3.2. Heater characterization LIG heater was obtained from ablation of KaptonTM polyimide. As seen in Figure S1A the heaters have a dimension of 10x15 mm with two contacts of Ag/Cl ink, keeping a heating surface of around 10x10 mm. The heaters was characterized physically and electrically to determine its composition and behaviour. To confirm the graphene nature of the material obtained, Raman spectroscopy was employed, whose results are shown in Figure S1B. As shown, the spectrum is composed by 4 peaks (D, G, 2D and D+G). The G (1570 cm-1) peak is related to the vibration of sp2 pairs of atoms, whereas the D (1341 cm-1 ) peak is associated to defects in the crystalline structure [38]. The 2D (2680 cm-1) peak, characteristic of graphene layers, is the result of second order resonant process. G+D peak also accounts for defects in the structure. The coexistence of D and 2D peaks demonstrate that the structure differs of a monolayer graphene [39]. Moreover, the structure has several defects in the crystalline structure, confirmed by an ID/IG ratio close to 1, and it is composed by several layers of graphene, explained by the ratio I2D/IG. The results show that the obtained material is derived from graphene, so it has some electrical conductivity. In Figure S1C and Figure S1D, SEM images of this heater are shown. As can be appreciated in the edge, laser changes the material for a uniform material with smooth surface to a porous irregular material. In detailed image this porosity can be appreciated more clearly. The temperature response of the heater was also measured by applying voltage steps with Precision Source/Measurement Unit B2902 while measuring temperature with IR camera Fluke TiS75 Figure S2A. As can be seen in Figure S2B, the setting time is around 7 seconds. Power density needed for each temperature is shown in Figure S2C, it varies from 0 to 1.4 W·cm-2 for temperatures from ambient to 300°C. Temperature vs voltage applied to the heater is shown in Figure S2D. Strategies, and Biomedical Applications,” Adv. Healthc. Mater., vol. 7, no. 4, p. 1700831, Feb. 2018. [16] S. Chandra, Y. Masuda, N. Shirahata, and F. M. Winnik, “Transition-Metal- Doped NIR-Emitting Silicon Nanocrystals,” Angew. Chemie Int. Ed., vol. 56, no. 22, pp. 6157–6160, May 2017. [17] J. G. Croissant, X. Cattoën, J.-O. Durand, M. Wong Chi Man, and N. M. Khashab, “Organosilica hybrid nanomaterials with a high organic content: syntheses and applications of silsesquioxanes,” Nanoscale, vol. 8, no. 48, pp. 19945–19972, 2016. [18] B. F. P. McVey and R. D. Tilley, “Solution Synthesis, Optical Properties, and Bioimaging Applications of Silicon Nanocrystals,” Acc. Chem. Res., vol. 47, no. 10, pp. 3045–3051, Oct. 2014. [19] T. Bose, Sandeep Ganayee, Mohd. Azhardin Mondal, Biswajit Baidya, Avijit Chennu, Sudhakar Mohanty, Jyoti Sarita Pradeep, “Synthesis of Silicon Nanoparticles from Rice Husk and their Use as Sustainable Fluorophores for White Light Emission,” ACS Sustain. Chem. Eng., vol. 6, no. 5, pp. 6203–6210, May 2018. [20] J. Zhang and S.-H. Yu, “Highly photoluminescent silicon nanocrystals for rapid, label-free and recyclable detection of mercuric ions,” Nanoscale, vol. 6, Mar. 2014. [21] Y. Zhong, Yiling Sun, Xiaotian Wang, Siyi Peng, Fei Bao, Feng Su, Yuanyuan Li, Youyong Lee, Shuit-Tong He, “Facile, Large-Quantity Synthesis of Stable, Tunable-Color Silicon Nanoparticles and Their Application for Long-Term Cellular Imaging,” ACS Nano, vol. 9, no. 6, pp. 5958–5967, Jun. 2015. [22] L. Mohapatra, Pratyasha Mendivelso-Perez, Deyny Bobbitt, Jonathan M. Shaw, Santosh Yuan, Bin Tian, Xinchun Smith, Emily A. Cademartiri, “Large-Scale Synthesis of Colloidal Si Nanocrystals and Their Helium Plasma Processing into Spin-On, Carbon-Free Nanocrystalline Si Films,” ACS Appl. Mater. Interfaces, vol. 10, no. 24, pp. 20740–20747, Jun. 2018. [23] G. A. Mastronardi, Melanie L. Hennrich, Frank Henderson, Eric J. Maier-Flaig, Florian Blum, Carolin Reichenbach, Judith Lemmer, Uli Kübel, Christian Wang, Di Kappes, Manfred M. Ozin, “Preparation of Monodisperse Silicon Nanocrystals Using Density Gradient Ultracentrifugation”, J. Am. Chem. Soc., vol. 133, no. 31, pp. 11928–11931, Aug. 2011. [24] X. Zhai, B. Song, B. Chu, Y. Su, H. Wang, and Y. He, “Highly fluorescent, photostable, and biocompatible silicon theranostic nanoprobes against Staphylococcus aureus infections,” Nano Res., vol. 11, no. 12, pp. 6417–6427, Dec. 2018. [25] Y. He, Yao Zhong, Yiling Peng, Fei Wei, Xinpan Su and S.-T. Lu, Yimei Su, Shao Gu, Wei Liao, Liangsheng Lee, “One-Pot Microwave Synthesis of Water- Dispersible, Ultraphoto- and pH-Stable, and Highly Fluorescent Silicon Quantum Dots,” J. Am. Chem. Soc., vol. 133, no. 36, pp. 14192–14195, Sep. 2011. [26] X. Zhong, Yiling Peng, Fei Bao, Feng Wang, Siyi Ji and Y. Yang, Liu Su, Yuanyuan Lee, Shuit-Tong He, “Large-Scale Aqueous Synthesis of Fluorescent and Biocompatible Silicon Nanoparticles and Their Use as Highly Photostable Biological Probes,” J. Am. Chem. Soc., vol. 135, no. 22, pp. 8350–8356, Jun. 2013. [27] Y. Zhong, Yiling Sun, Xiaotian Wang, Siyi Peng, Fei Bao, Feng Su, Yuanyuan Li, Youyong Lee, Shuit-Tong He, “Facile, Large-Quantity Synthesis of Stable, Tunable-Color Silicon Nanoparticles and Their Application for Long-Term Cellular Imaging,” ACS Nano, vol. 9, no. 6, pp. 5958–5967, Jun. 2015. [28] Y. Zhong, Yiling Peng, Fei Wei, Xinpan Zhou, Yanfeng Wang, Jie Jiang, Xiangxu Su, Yuanyuan Su, Shao Lee, Shuit-Tong He, “Microwave-Assisted Synthesis of Biofunctional and Fluorescent Silicon Nanoparticles Using Proteins as Hydrophilic Ligands,” Angew. Chemie Int. Ed., vol. 51, no. 34, pp. 8485– 8489, Aug. 2012. [29] G. Chen, Haoyu Wu, Li Wan, Yuqi Huang, Lulu Li, Ningxing Chen, Jinyang Lai, “One-step rapid synthesis of fluorescent silicon nanodots for a hydrogen peroxide-related sensitive and versatile assay based on the inner filter effect,” Analyst, vol. 144, no. 13, pp. 4006–4012, 2019. [30] C. Li et al., “Flexible graphene electrothermal films made from electrochemically exfoliated graphite,” J. Mater. Sci., vol. 51, no. 2, pp. 1043–1051, Jan. 2016. [31] S. Xie, T. Li, Z. Xu, Y. Wang, X. Liu, and W. Guo, “A high-response transparent heater based on a CuS nanosheet film with superior mechanical flexibility and chemical stability,” Nanoscale, vol. 10, no. 14, pp. 6531–6538, 2018. [32] K. Handique, “Microfluidic cartridge and method of making same,” US8709787B2, 2004. [33] A. C. Catto et al., “An easy method of preparing ozone gas sensors based on ZnO nanorods,” RSC Adv., vol. 5, no. 25, pp. 19528–19533, 2015. [34] N. Romero, Francisco J. Rivadeneyra, Almudena Ortiz-Gomez, Inmaculada Salinas, Alfonso Godoy, Andrés Morales, Diego P. Rodriguez, “Inexpensive Graphene Oxide Heaters Lithographed by Laser,” Nanomaterials, vol. 9, no. 9, p. 1184, Aug. 2019. [35] M. R. Bobinger et al., “Flexible and robust laser-induced graphene heaters photothermally scribed on bare polyimide substrates,” Carbon N. Y., vol. 144, pp. 116–126, Apr. 2019. [36] I. Ortiz-Gomez et al., “A vinyl sulfone clicked carbon dot-engineered microfluidic paper-based analytical device for fluorometric determination of biothiols,” Microchim. Acta, vol. 187, no. 7, p. 421, 2020. [37] M. Basiaga, Z. Paszenda, W. Walke, and J. Karasiński Pawełand Marciniak, “Electrochemical Impedance Spectroscopy and Corrosion Resistance of SiO2 Coated CpTi and Ti-6Al-7Nb Alloy,” in Information Technologies in Biomedicine, Volume 4, 2014, pp. 411–420. [38] F. Tuinstra and J. L. Koenig, “Raman Spectrum of Graphite,” J. Chem. Phys., vol. 53, no. 3, pp. 1126–1130, Aug. 1970. [39] A. C. Ferrari et al., “Raman Spectrum of Graphene and Graphene Layers,” Phys. Rev. Lett., vol. 97, no. 18, p. 187401, Oct. 2006. [40] H. Chen et al., “One-step rapid synthesis of fluorescent silicon nanodots for a hydrogen peroxide-related sensitive and versatile assay based on the inner filter effect,” Analyst, vol. 144, no. 13, pp. 4006–4012, 2019. [41] B. Sharma and S. Tanwar, “One Pot Green Synthesis of Si Quantum Dots and Catalytic Au Nanoparticle-Si Quantum Dot Nanocomposite,” ACS Sustain. Chem. Eng., vol. 7, Jan. 2019. [42] Y. Qi, Y. Chen, J. He, and X. Gao, “Highly sensitive and simple colorimetric assay of hydrogen peroxide and glucose in human serum via the smart synergistic catalytic mechanism,” Spectrochim. Acta Part A Mol. Biomol. Spectrosc., vol. 234, p. 118233, 2020. [43] D. O. F. Kidney, “Laboratory Assessment of Kidney Disease,” Pocket Companion to Brenner Rector’s Kidney, pp. 21–41, 2011. [44] F. Della Pelle, A. Scroccarello, S. Scarano, and D. Compagnone, “Silver nanoparticles-based plasmonic assay for the determination of sugar content in food matrices,” Anal. Chim. Acta, vol. 1051, pp. 129–137, 2019. Table 1. Analytical characteristics of µPAD for glucose or fructose determination. Analytical parameter Values for glucose Values for fructose Measurement range, µM 2.68 – 200.00 1.55 – 100.00 Slope 0.51 0.79 Intercept 20.56 6.82 LOD, µM 0.80 0.51 LOQ, µM 2.68 1.55 Precision, % 40 µM 2.64 - Precision, % 100 µM 1.84 - Table 2. Determination of glucose in human urine samples. Sample Found, µM Added, µM Total found, µM Recovery, % Urine 1 25.56 10.00 36.53 109.70 20.00 46.07 102.55 30.00 55.33 99.23 Urine 2 30.90 10.00 41.49 105.90 20.00 53.66 113.80 30.00 61.94 103.46 Serum - 10.00 10.74 107.40 20.00 19.47 97.33 30.00 30.27 100.92 50.00 50.00 99.99 Table 3. Determination of total carbohydrates in commercial juices and teas (n = 9). Samples Labelled g·mL - 1 Found g·mL - 1 Pineapple juice 0.026 0.02 ± 0.003 Orange juice 0.102 0.09 ± 0.011 Tomato juice 0.035 0.03 ± 0.006 Black tea 0.045 0.04 ± 0.003 Green tea 0.082 0.07 ± 0.002 Figure captions Figure 1. Hardware characteristics. (A) Board dimensions and distribution; (B) Folder state of the board inside the housing; (C) Housing made for the board; (D) Microfluidic paper-based analytical device for determination total carbohydrates with synthetized SNDs; (E) Portable housing accomplished to the smartphone. Figure 2. Schematic illustration of SNDs synthesis from APTS and carbohydrate. Figure 3. Calibration curve for (A) glucose and (B) fructose. Conditions: 1 µL APTS; heating at 80ºC for 30 min; 7.5 µL of glucose or fructose solutions; λexc= 365 nm. Data points are the mean of 3 assays Figure 4. Response of different interferences and carbohydrates. Conditions: 1 µL APTS; heating at 80ºC for 30 min; 7.5 µL of interference solutions 250 µM; λexc= 365 nm. Data points are the mean of 3 assays. Figure 1. Hardware characteristics. (A) Board dimensions and distribution; (B) Folder state of the board inside the housing; (C) Housing made for the board; (D) Microfluidic paper-based analytical device for determination total carbohydrates with synthetized SNDs; (E) Portable housing accomplished to the smartphone. Figure 2. Schematic illustration of SNDs synthesis from APTS and carbohydrate.